  • In this video we made an anode of precious metals containing alloys and elements. From the anode we extracted and refined palladium, gold and silver.
    #gold #preciousmetals #palladium #silver #owltech
  • НаукаНаука

Комментарии • 215

  • @NormReitzel
    @NormReitzel Год назад +7

    From a career chemist and someone who taught chemistry at UTSA, the easiest recovery of silver from AgCl is to air dry the AgCl, then just mix 1:1 by weight of AgCl and soda ash, put in graphite crucible and melt, you can then pour off beautiful silver metal, easy peasy. No need to reduce the salt or oxide beforehand. Nice presentation.

    • @OwlTech333
      @OwlTech333  Год назад +1

      Thanks, usually I melt the silver chloride with caustic soda but wanted to try something different for the video

    • @Tyresio12
      @Tyresio12 10 месяцев назад +1

      What are the losses of AgCl during melting, since it's somewhat volatile (like many chlorides)?
      Certainly this method is easy, but does it provide the some recovery?

    • @OwlTech333
      @OwlTech333  10 месяцев назад +1

      @@Tyresio12 no losses, if you heat AgCl under NaOH, basically you are converting the silver chloride to silver oxide which decomposes to silver metal and oxygen at around 300C

    • @erikreber3695
      @erikreber3695 2 месяца назад

      Hmmm. I hope I find this useful one day as I am processing my scrap now.

  • @WaffleStaffel
    @WaffleStaffel 2 года назад +6

    29:40 -haha, the panic in those shaking hands. We've all been there once or twice.

  • @julianalcorso5703
    @julianalcorso5703 Год назад +2

    Just watched it again! Bloody brilliant!!

  • @ap.h.y.m4942
    @ap.h.y.m4942 Год назад +3

    Excellent method, organized, clean and clear. Excellent. Thank you very much. You are a wonderful teacher

  • @jameygeimer423
    @jameygeimer423 10 месяцев назад +2

    Great videos! You showed how to separate my favorite metals. Very informative as always. I'm a big fan!

  • @coreygold1923
    @coreygold1923 2 года назад +6

    Ah hahaha. You did such a good job on these buttons that I was finally able to see your face in the reflection .😀 very very nice 👌👍👏😀

  • @irlans2042
    @irlans2042 Год назад +1

    Nice result.
    Good job. 👍👍👍
    Thank's for the video.

  • @SURFEAMORETERNO
    @SURFEAMORETERNO 2 года назад +7

    Greatly improved the presentation of the video with things in a better organized way.
    Congratulations and thanks for yet another beautiful demonstration.

  • @bbbruh8809
    @bbbruh8809 7 месяцев назад +2

    Best refiner on yt

  • @2001pulsar
    @2001pulsar 2 года назад +1

    A long journey, with a prize at the end.
    Very nice.

  • @razor1983
    @razor1983 2 года назад +2

    Artist at work!!!

  • @lucianodipietro7933
    @lucianodipietro7933 Год назад +1

    Grazie e complimenti per il riutilizzo del bel barattolo di vetro della "nutella" famosa cioccolata italiana. 😀

  • @jaimejuarez466
    @jaimejuarez466 2 года назад +2

    Todo un maestro!!

  • @OnsloVest
    @OnsloVest 2 года назад +3

    Nice one mate! Amazing Pd result!

  • @hiteshmorzaria7254
    @hiteshmorzaria7254 2 года назад +1

    Very Nice 👍 . Glad to see like this result.

  • @zafarazmi7599
    @zafarazmi7599 2 года назад +2

    I m very happy long time back 👍👍👍👍

  • @escrapchannel
    @escrapchannel 2 года назад +1

    Epic video 🌟 🌟 🌟 🌟 🌟 👍

  • @serjgarelii866
    @serjgarelii866 2 года назад +5

    Метод с паладозамином и мур.кислота интересен! Не знал о таком варианте, спасибо за информацию!!!

    • @rosenraykov3136
      @rosenraykov3136 2 года назад +1

      Это является классическим способом аффинажа.

    • @user-sd1ur4bn2r
      @user-sd1ur4bn2r Год назад

      @@rosenraykov3136 Да это ОНО лизнуло ради лайка))

  • @tinsoffish1810
    @tinsoffish1810 2 года назад +3

    For some reason the nuttella labware is hilarious 😂😂😂

  • @tortugakourosh6805
    @tortugakourosh6805 2 года назад +1

    Bonjour qu'elle plaisir de vous revoir superbe vidéo .
    Merci pour la traduction 👍

    • @OwlTech333
      @OwlTech333  2 года назад

      Salut! Merci d'avoir regardé!

  • @jamisontaylor878
    @jamisontaylor878 2 года назад +2

    Excellent video thank you 😊

  • @muchl8006
    @muchl8006 Год назад +1

    I was vibing the whole vid. Well done

  • @anisahemad6968
    @anisahemad6968 2 года назад +1

    Very very nice

  • @hayderalkhafaji8408
    @hayderalkhafaji8408 2 года назад +1

    Nice well done sir

  • @royalrefining6182
    @royalrefining6182 2 года назад +3

    Flawless Pd button mate. Great refiner

  • @jaimejuarez466
    @jaimejuarez466 2 года назад +1

    Te quedó muy bien!!

  • @platinumskies7968
    @platinumskies7968 2 года назад +1

    Great vid thanks

  • @kaanates
    @kaanates Год назад +2

    Hello
    I think you survived by boiling the gold precipitated by tin and lead with sulfuric acid (?)
    What should be done if the solution was nickel and solder?
    Or is there a pre-cleaning method you would recommend to get rid of tin, nickel, solder and lead in the first place?
    Respects

  • @ap.h.y.m4942
    @ap.h.y.m4942 Год назад

    If I don't find formic acid, can I separate the yellow powder from the dilute hydrochloric acid, then wash it with distilled water, then melt it directly?

  • @goldscrapurbanmining
    @goldscrapurbanmining 2 года назад +1

    business in Korea. Your video is always helpful during electronic scrap-related RUclips broadcasts. Thank you.

  • @krazygold18
    @krazygold18 2 года назад +3

    СОВА всегда оригинален ЛАЙК

  • @user-xx5ij9zc5s
    @user-xx5ij9zc5s 2 года назад +2

    Ну ты могёшь 👍👍👍🤝💪

  • @moshinsiddique6001
    @moshinsiddique6001 2 года назад

    Sir would you please tell me how to recover platinum from the carbon catalyst black powder

  • @bbbruh8809
    @bbbruh8809 7 месяцев назад +2

    Btw what if those contact points have cadmium present, would it change the reaction or your refining process?

    • @OwlTech333
      @OwlTech333  7 месяцев назад +1

      I know for sure that they don’t

    • @bbbruh8809
      @bbbruh8809 7 месяцев назад +1

      @@OwlTech333 thank you for quick response, much appreciated

  • @niculanicolaeofficial9114
    @niculanicolaeofficial9114 2 года назад +1

    Great one. So the Cooper was lost after Amonia, and HCL was aded, and paladium salt was left in filter, right?

  • @CARLOSCESPEDESbiocihealth
    @CARLOSCESPEDESbiocihealth 2 года назад

    Can someone recommend me how to leach mineral concentrates that contain elements of the platinum group such as Rh, Pt, Pd, Ir in the metallic state or sulfides or oxides.??

  • @TrinityGoldRecovery
    @TrinityGoldRecovery 2 года назад +1

    3times I watching this videos...

  • @hmwatercomponentspvtltd2108
    @hmwatercomponentspvtltd2108 2 года назад +1

    Hi, would you please explain making of RuCl3 from ruthinium sponge?
    Thank you

  • @svenp6504
    @svenp6504 2 года назад

    Great video! If there was Pt present, where would it have ended up? With the Au or the Pd?

    • @OwlTech333
      @OwlTech333  2 года назад

      Some with the au and some in the filter paper @19:00

  • @miguelangelvegamoreno5249
    @miguelangelvegamoreno5249 2 года назад +1

    Muy especial.tu travajo.

  • @tinsoffish1810
    @tinsoffish1810 2 года назад +1

    Incredible😃!!....now to sort the dirty button!!

    • @OwlTech333
      @OwlTech333  2 года назад +1

      Next time with the other batch

    • @tinsoffish1810
      @tinsoffish1810 2 года назад

      @@OwlTech333 congradulations on the 100%💯⚫☜pure,shiney pd!!

    • @OwlTech333
      @OwlTech333  2 года назад

      @@tinsoffish1810 Thank you!

  • @varlov5523
    @varlov5523 2 года назад +1

    здраствуйте ув. сова благодарность за видео. от души;)

    • @OwlTech333
      @OwlTech333  2 года назад +1

      Спасибо за просмотр!

    • @varlov5523
      @varlov5523 2 года назад

      @@OwlTech333 нет проблем.

    • @varlov5523
      @varlov5523 2 года назад

      @@OwlTech333 хороший результат и обстановка в лаборатории тоже:)

  • @billsmathers7787
    @billsmathers7787 2 года назад +1

    What is the composition of Vokelen's salt? I havent been able to find any information about it. What metal does it contain?

    • @OwlTech333
      @OwlTech333  2 года назад +4

      "palladium compound ([Pd(NH3)4PdCl4]) is known as "Vauquelin’s salt"
      pubs.rsc.org/en/content/articlelanding/1932/jr/jr9320001895/unauth

    • @jesserodgers2812
      @jesserodgers2812 Год назад

      Pretty sure I ran into some of this recently, although I didn't know it existed and instead took it for an Mn salt. Gonna have to do some tests on my waste from that project.

  • @RidJam2
    @RidJam2 Год назад

    What kind of gas burner do you use for melting your palladium??

  • @tawnihaynie1065
    @tawnihaynie1065 2 года назад +1

    Great video. I love it. Have a nice day. Talk to you later my friend. 🙂🙂🙂😇😇😇👍👍👍❣❣❣❤❤❤

  • @salihakdag6371
    @salihakdag6371 Год назад +1

    Emeğine sağlık çok güzel video.Büyük geçmiş olsun tehlikeden kıl payı kurtuldun. ALLAH KORUDU .BAŞARILAR.

  • @user-fw6lm4yx2q
    @user-fw6lm4yx2q Год назад

    If hydrochloric acid is diluted in a solution filtered with ammonia water, is it a different substance from ammonium chloride?
    Does platinum react with ammonia water-hydrochloric acid?

  • @hasantokgoz3069
    @hasantokgoz3069 2 года назад +1

    Sağol kardeşim Allah razı olsun senden teşekürler sana

  • @user-sd1ur4bn2r
    @user-sd1ur4bn2r 9 месяцев назад +2

    Икра черная))

  • @jorgealbertovelasquez9669
    @jorgealbertovelasquez9669 Год назад +1

    10/10 my teacher

  • @mahmmud980
    @mahmmud980 2 года назад +2

    very good professional
    Would it not be better to deposition palladium with DMG and then treat it with DMG precipitate with formic acid? The steps were shorter and easier, and would you give the same result?

    • @OwlTech333
      @OwlTech333  2 года назад +2

      I wont be able to get it that pure with DMG straight

  • @andredesouzadasilva5597
    @andredesouzadasilva5597 Год назад

    Posso substituir ácido fórmico, por formol?

  • @khanacknowledge7604
    @khanacknowledge7604 Год назад +2

    What will be solution temperature When you adding 20% ammonia ? Is it cool down or hot solution?

    • @OwlTech333
      @OwlTech333  Год назад +1

      It’s cool but since the reaction is exothermic it heats up quickly, it should be heated further until all pink precipitate dissolve. Then should be left to cool before filtration.

    • @khanacknowledge7604
      @khanacknowledge7604 Год назад +1

      @@OwlTech333 many thanks.

  • @julianalcorso5703
    @julianalcorso5703 2 года назад +2

    Hey Owl, Great Vid. Your best yet I reckon. Love your new set-up, New lighting, and new camera?? Well done you!! Just a thought but right at the beginning would it not have been easier and a lot quicker to just pour the melted alloys into cold water to make flakes? These dissolve very quickly and easily. Keep up the great work.

    • @OwlTech333
      @OwlTech333  2 года назад +1

      Actually a thin sheet dissolves much much quicker than shots and I've learned this from expedience. I don't know why... Shots have much larger surface area...

    • @julianalcorso5703
      @julianalcorso5703 2 года назад

      @@OwlTech333 will try this on my next refining. Thanks!

    • @Scola9895
      @Scola9895 2 года назад

      New setup, new lighting, new camera but still no gloves nor eyes protection 👍

    • @shawnsmith9512
      @shawnsmith9512 8 месяцев назад

      It is easier, but it is not quicker and you will have more residuals. Cast and roll is the by the book method and the best bang for the buck.

  • @user-fw6lm4yx2q
    @user-fw6lm4yx2q Год назад

    What percentage of formic acid do you use?

  • @masteroogwayy0339
    @masteroogwayy0339 2 года назад +1

    Does this process produce mercury during extraction

  • @tomspeed2000
    @tomspeed2000 2 года назад +1

    I had more than 15l solution with containing all those metals;))its more than 2 weeks that im so lazy to filtering ..

    • @jakospence
      @jakospence Год назад

      Put it in a 5000ml beaker on an electric griddle and put some kaowool on the unused surface and on the sides of the beaker. It minimizes waste of electricity because the heat will only go through the beaker, and it will prevent having to re-evaporate what condenses on the walls of the beaker and rolls back down into solution.
      That’s how I concentrate my waste for subsequent recovery!

  • @chosen1one930
    @chosen1one930 2 года назад +1

    I finally got some USSR material, flat ICs with legs parallel to the floor and gold caps on top and bottom. I'll have to send you a picture through email I don't have a clue what they yield and selling on eBay can usually yield a bigger payday, or equal to the gold yield

  • @user-ed5wv7fb3y
    @user-ed5wv7fb3y 2 года назад +2

    Круто 👍

  • @ChimeraChemLab
    @ChimeraChemLab Год назад +2

    Я как-то раз тоже сплавил всё в кучу (там, правда, были только серебро, медь, немного золота и припоя после неудачных очисток). Результат мне не понравился, потом это сложно разделить, у меня получились высокие потери

  • @viyuy74
    @viyuy74 Год назад

    Se ven muy interesantes sus videos felicidades se ve que si sabe lo que hace.¿ como separaría plata y bismuto disuletos en ácido nítrico ? Ya que se precipitan igual con la sal o Nacl. Y sigue contaminada la plata.muchas gracias pr su atención.

  • @sabarlaras2700
    @sabarlaras2700 2 года назад

    halo..ijin bertanya Master...
    apakah metode ini bisa di coba dalam matrial batuan sufida yg terkontaminasi cenderung lebih banyak unsurr Fe,cu,zn,pb,all,dll...
    terutama unsur sufidanya...mohon penjelasan Master..Tanks..

  • @miguelangelvegamoreno5249
    @miguelangelvegamoreno5249 2 года назад

    Yo tengo un predio con platino y Au y no se como prosesarlo .

  • @ap.h.y.m4942
    @ap.h.y.m4942 Год назад +1

    En el minuto 15:58 del video, si agregamos ácido sulfúrico en lugar de ácido sulfámico para precipitar el plomo, ¿funcionará?

  • @mahmmud980
    @mahmmud980 2 года назад +1

    welcome

  • @GEMSTATEGOLDNSILVER
    @GEMSTATEGOLDNSILVER Год назад +1

    Absolute Kick Ass!

  • @goldandsilverminingintheci8942
    @goldandsilverminingintheci8942 2 года назад +1

    Nice. I send my precious metals to a refiner. I can't refine where I'm at. I have a small channel where I sort gold and silver.

  • @whatwill1812
    @whatwill1812 2 года назад +1

    Sir i hv 50kg blue type mlcc and 25+non magnetic mlcc..both removed from old japan NEC telecommunication card..if u hv any idea how much pd recovery from that

    • @OwlTech333
      @OwlTech333  2 года назад

      about 0.5kg Pd if they are similar to ruclips.net/video/8MdnhlxKlH0/видео.html

    • @whatwill1812
      @whatwill1812 2 года назад +2

      😀😀 thanks

    • @scrappydoo7887
      @scrappydoo7887 2 года назад

      @@whatwill1812 do you mean resin dipped?

    • @RizwanKhan-bi1ki
      @RizwanKhan-bi1ki 2 года назад +1

      Good job.

  • @Kinneycc123
    @Kinneycc123 2 года назад +1

    What are you putting in the mold to get it to release so easily?

  • @tonghongquyen2093
    @tonghongquyen2093 2 месяца назад +1

    vàng .bạc .pd.và tách ra từng kim loại một.

  • @blackcrow6110
    @blackcrow6110 2 года назад

    ДМГ выделяет платину ??

  • @user-wu7mp8tg2g
    @user-wu7mp8tg2g 2 года назад +4

    👍тоже так делаю , укажу на небольшие ошибки после аммиака при добавлении соляной кислоты стакан не надо охлаждать надо немного подогревать ,тогда вываливается полностью.при восстановлении не надо много муравьиной надо немного соды или каплю гидрозин гидрата ,промывать кипятком несколько раз

    • @rosenraykov3136
      @rosenraykov3136 2 года назад +1

      Напротив,точно надо охлаждать и соблюдать от 0 до 10 градусов Цельсия и пха не ниже 1,5,если нагревать,то часть палладозамина превращается в тетрахлорпалладат аммония,читайте по больше книжек

    • @user-wu7mp8tg2g
      @user-wu7mp8tg2g 2 года назад

      @@rosenraykov3136 книжки книжками а на практике по другому

    • @rosenraykov3136
      @rosenraykov3136 2 года назад

      @@user-wu7mp8tg2g Когда ты получишь пару килограммов палладия,как меня,тогда и будешь советовать.....

    • @user-wu7mp8tg2g
      @user-wu7mp8tg2g 2 года назад

      @@rosenraykov3136 ты крут не по годам

  • @gold_turkey
    @gold_turkey 2 года назад

    Turkiye den selamlar,başarilar dilerim,100 gram cevher, xrf sonuclari %6 rodium %5 paladium,bunu en verimli hangi proses ile islemeliyiz

  • @tamassandor478
    @tamassandor478 4 месяца назад +1

    Hello! Very good video! What pH should the formic acid be adjusted to?

  • @battleshippotemkin560
    @battleshippotemkin560 2 года назад +2

    Наверное выделить серебро из хлорида было бы проще куском алюминиевой проволоки. Без расхода щелочи и муравьиной кислоты.

  • @wundw
    @wundw 2 года назад +1

    Pretty coole 👌👍👏😀

  • @user-we7dw5ox6s
    @user-we7dw5ox6s 2 года назад +1

    Очень круто👀👍

    • @OwlTech333
      @OwlTech333  2 года назад

      Спасибо!

    • @user-we7dw5ox6s
      @user-we7dw5ox6s 2 года назад +1

      @@OwlTech333 это вам спасибо!!!с таким ахуеннным удовольствием посмотрел ваш ролик много ощущений пережитых вспомнил.

  • @scrappydoo7887
    @scrappydoo7887 2 года назад +2

    You got 100% purity on the palladium!?

    • @OwlTech333
      @OwlTech333  2 года назад +2

      yes

    • @scrappydoo7887
      @scrappydoo7887 2 года назад

      @@OwlTech333 well done 👍 it's usually hard to not have at least the slightest bit of contamination from other PGMs

  • @azizekurtametova7250
    @azizekurtametova7250 2 года назад +2

    Привет удачи и здоровья

  • @ralitzaboteva3751
    @ralitzaboteva3751 2 года назад +1

    😲😁

  • @tejosupeno4106
    @tejosupeno4106 2 года назад

    Air nya pakai air apa?.. Trimas

  • @SocratePrimusSapiens
    @SocratePrimusSapiens 2 года назад +2

    Great Job !
    Beautiful Pd bead !!
    It's always a great fun to get a nice reward especially when you know the time we spent on "collecting" before...
    But His-tory and fake money are not in perfect condition those days...
    Time to keep Faith in Freedom of prices.
    Whish you the Best for the year !

  • @NormReitzel
    @NormReitzel Год назад +1

    Like your videos, Except, the background "Music" is Horrid.

  • @haidthaidr4725
    @haidthaidr4725 2 года назад +1

    سلام عليكم اخي العزيز يوجد عندي ماء مالكي يوجد فيه هب لا يرسب بسبب الرصاص والقصدير كيف تخلص من الرصاص او القصدير ارجو الرد اخي العزيز

  • @shaikjamaluddinnazeema8600
    @shaikjamaluddinnazeema8600 2 года назад +1

    👌👏👏👏💐🙏🙏🌹

  • @user-cr9ly9wh4s
    @user-cr9ly9wh4s 2 года назад +1

    Интересненько. Уже объёмы не такие большие. К сожалению. 🙄

    • @OwlTech333
      @OwlTech333  2 года назад

      есть количества, много видео тоже

  • @susysusilowatisari6479
    @susysusilowatisari6479 2 года назад +1

    TOO complicated process owl. But thanks for fun.
    Why after silver take it didn't precipitaded solution with chemical solution.

  • @Modestas19920
    @Modestas19920 5 месяцев назад

    lead recovery video ?

  • @romanpankin5412
    @romanpankin5412 2 года назад +1

    Это сплав Доре,перерабатывал такой только еще и с платиной.Очень муторное занятие несмотря на кажущуюся простоту.

    • @OwlTech333
      @OwlTech333  2 года назад

      Так точна

    • @user-ex8wu4fn3z
      @user-ex8wu4fn3z 2 года назад +2

      Как платину от палладия отделял?

    • @OwlTech333
      @OwlTech333  2 года назад

      @@user-ex8wu4fn3z платины не было, а если бы была, то разделяли бы хлористым аммонием

    • @user-ex8wu4fn3z
      @user-ex8wu4fn3z 2 года назад +1

      @@OwlTech333 не всё так просто))))особенно на объёме..

    • @user-ex8wu4fn3z
      @user-ex8wu4fn3z 2 года назад +1

      @@OwlTech333 ещё когда в аммиак солянку добавляешь,можно положить в аммиак лед(подготовленный из дистилята)тогда меньше палладия в остатке ...

  • @thecelticprince4949
    @thecelticprince4949 2 года назад +1

    protective gloves will go long way to protect your hands from all those nasty chemicals.

  • @alexhsabro2028
    @alexhsabro2028 2 года назад +2

    Ну и алхимики.Выкрутились. Следущее видео про филосовский камень, надеюсь?

  • @yuryandy861
    @yuryandy861 2 года назад +1

    Еще бы русские субтитры было бы вообще супер 🤗

    • @OwlTech333
      @OwlTech333  2 года назад

      сделал уже

    • @yuryandy861
      @yuryandy861 2 года назад

      @@OwlTech333 thank you very much, my mother said learn english sonny 😁😁😁

  • @user-we7dw5ox6s
    @user-we7dw5ox6s 2 года назад +1

    А как с фильтрами работали не показали а это было бы познавательно посмотреть.

    • @OwlTech333
      @OwlTech333  2 года назад

      в следующий раз

  • @zekeriyaguner7646
    @zekeriyaguner7646 Год назад

    Çok güzel anlatıyon

  • @pixelpatter01
    @pixelpatter01 8 месяцев назад +1

    Be careful of the vapors from melting random electrical parts. A little Beryllium in a bronze spring or relay reed and you will be very sorry and very sick.

    • @bbbruh8809
      @bbbruh8809 7 месяцев назад

      Always wear ppe face shield and respirator!
      It's obvious

    • @bbbruh8809
      @bbbruh8809 7 месяцев назад

      Also have Hume hood or outside

  • @ArturoQuintero-fr8wb
    @ArturoQuintero-fr8wb Год назад +1

    Hola presentelo en es pañol

  • @sddirt6840
    @sddirt6840 4 месяца назад

    This is the most time-consuming way to do this.

  • @alligator8811
    @alligator8811 2 года назад +2

    Спасибо за видео. Жалко что в этом видео субтитров на русском языке нет.

    • @OwlTech333
      @OwlTech333  2 года назад +5

      Будет

    • @alligator8811
      @alligator8811 2 года назад +1

      @@OwlTech333 Будем ждать!

    • @OwlTech333
      @OwlTech333  2 года назад +4

      @@alligator8811 уже есть

  • @diamond.hgp.
    @diamond.hgp. 2 года назад +1

    Bạn đốt chúng bằng khí Hydro.?.

    • @OwlTech333
      @OwlTech333  2 года назад +1

      không, oxy và propan

  • @anakrantau3935
    @anakrantau3935 2 года назад +1

    Apakah itu amoniak untuk kue

    • @OwlTech333
      @OwlTech333  2 года назад

      itu adalah amonia NH4OH

    • @anakrantau3935
      @anakrantau3935 2 года назад

      @@OwlTech333 maaf sir apa yg anda gunakan untuk mengendapkan Palladium ?

    • @OwlTech333
      @OwlTech333  2 года назад

      @@anakrantau3935 HCl asam hidroklorik