  • What metal comes to mind when you hear “precious metal”, gold, platinum, silver? Lead comes to mind when I hear “precious metals”. Lead is a highly dynamic metal that can be used to make anything from fishing sinkers to ammunition.
    In this episode I’m going to teach you the basic steps to processing scrap lead wheel weights into cleaner more pure lead ingots that can be used to make whatever your heart desires.
    Links for products used:
    -single propane burner: amzn.to/48XAXV1
    -cast iron pot: amzn.to/3SlDrYb
    -serving spoon set: amzn.to/48v8ztI
    -metal dross bucket: amzn.to/427yqpm
    -lead mold: amzn.to/3tUuIT8
    -muffin tin mold: amzn.to/3O5GJMF
    -leather gloves: amzn.to/4aVVR94
    -3m respirator: amzn.to/4aZnG07
    -propane torch: amzn.to/48RFZ5B
    -safety glasses: amzn.to/3tLNEUh
    -lead casting pot: amzn.to/3O1HiH6
    If you have any questions or would like to get into contact with me feel free to reach out at:
    eternalfishquest@gmail.com
    / fishquest
    ⬆️⬆️ SUBSCRIBE HERE
    -Travis Johnson
    Fish Quest
  • КиноКино

Комментарии • 51

  • @mcdouche2
    @mcdouche2 5 месяцев назад +5

    I LOVE how this guy pluralizes words that don't need it. Constitutions, ammunitions.....Just like Kenny Powers! I think its endearing and I share this man's outlook on the future of America!

    • @FishQuest
      @FishQuest  5 месяцев назад +2

      The noun ammunition can be countable or uncountable. In more general, commonly used, contexts, the plural form will also be ammunition. However, in more specific contexts, the plural form can also be ammunitions e.g. in reference to various types of ammunitions or a collection of ammunitions.
      Constitutions referring to the potential that the viewers of this particular video are not of the same nationality, but rather scattered in various countries in which “constitutions” would be proper.
      Thanks for the comment and keeping me honest on my 3rd grade grammar.

    • @mcdouche2
      @mcdouche2 5 месяцев назад

      @@FishQuest Kenny, just own it. When speaking of ammo, we don’t say ammunitions. We say ammo, or ammunition. Regardless of caliber or lot.
      Also, there is only one REAL constitution.
      Thank bro, we know what time it is on the street. FJB.

  • @outdoorinterests
    @outdoorinterests Год назад +2

    Absolutely agree.
    They won't stop us.

  • @sirspark-a-lot8782
    @sirspark-a-lot8782 5 месяцев назад +2

    Great informative video. I especially like your use of a shovel to add to the molten pool.

    • @FishQuest
      @FishQuest  5 месяцев назад

      Hey thanks for the feedback, it didn’t take long to realize that wheel weights buried in a 5 gallon bucket may hold some water which will pop explosively when it submerges in lead, the shovel is a must now a days hah.

  • @alexandraf11
    @alexandraf11 4 месяца назад +2

    Thanks for posting this ❤

    • @FishQuest
      @FishQuest  4 месяца назад

      For sure, thanks for subscribing!

  • @noelguerrero3018
    @noelguerrero3018 11 месяцев назад +9

    I used these with the Team Catfish weight slides to make a ruclips.net/user/postUgkxdmsDj7fQXe77DC0l7P7ua8B3PiESUubM Carolina rig and they were perfect for the ponds I fish. I have also used them to make 3 way rigs and these work perfectly. Haven't had any issues with them snagging in rocks or in weeds yet.

  • @danielsbackforty8094
    @danielsbackforty8094 Год назад +1

    Great video!! 👍 Thanks for info! Very good content brother! 👌

    • @FishQuest
      @FishQuest  Год назад

      Thanks for the feedback! I greatly appreciate it!

  • @shadowcastre
    @shadowcastre Год назад +4

    A well done video..!
    I will give you a clarification though. Moisture is only a problem when it gets beneath the surface of the melt. Any moisture on top will simply hiss & steam away. Also.. Sawdust is an excellent flux but you need to let it completely char before stirring it in. It could contain moisture and then we are back to the water & molten lead discussion.
    Thanks for the video...

    • @FishQuest
      @FishQuest  Год назад +1

      Thanks for the comment, all excellent, noteworthy points.

  • @smsgtbulldog
    @smsgtbulldog Год назад +1

    Great video 👍🏻👍🏻

  • @josephjohnson9802
    @josephjohnson9802 2 года назад +1

    Do you have any links to products you use that you have found more efficient than others?!

  • @fragnicht1734
    @fragnicht1734 Год назад +1

    I agree with everything you have said in this video

  • @RustyInventions-wz6ir
    @RustyInventions-wz6ir 7 месяцев назад +1

    Just found your channel and Subscribed. Very nice

    • @FishQuest
      @FishQuest  6 месяцев назад

      @RustyInventions-wz6ir, welcome aboard and thank you.

  • @johnhoward7298
    @johnhoward7298 4 месяца назад

    Great explanation of how to process lead . Thanks .
    How do You dispose of the waste ?

    • @FishQuest
      @FishQuest  4 месяца назад

      thank you and great question. In the past, I waited until the waste had cooled and then I put it into the dumpster. More recently I've been taking the cooled waste to a recycling center where they'd take it for free.

  • @ITZGR82BFREE
    @ITZGR82BFREE 4 месяца назад +1

    Excellent video. I notice you don't seperate the soft lead into a seperate batch. Also you need to address the ZINC weights that are always in the mix, and the importance of seperating them out. I know that you know this but just didn't mention it. ZINC melts at a higher temp so if you DON'T let your batch get too hot they will get scraped out with the steel clips. BUT, if you let your batch get above 667 degrees, any stray zinc weights will melt and destroy the entire batch. ZINC will melt into the lead but will not alloy with it. ZINC contamination forms a gloopy ugly mess that is useless. Again great video, thanx.

    • @FishQuest
      @FishQuest  4 месяца назад

      great comment and info. looking back, I wish I would have gone over the need to sort out the zinc wheel weights from the mix or make mention of the need to babysit the melting pot to spot any stray zinc weights. Looking back I don't believe I have ever actually melted zinc weights on my lead because I'm constantly watching and waiting for the lead to melt so the zinc didn't have the chance to melt at a higher temp. From what I understand only a percentage of the zinc will mix yet it will "poison" the batch which will result in inferior casts. I do have one question for you and that is lead melts at 621 °F and zinc at 786 °F, you mentioned 667°F, what does that temp pertain to?
      Again thanks for the comment and helping others learn.

    • @ITZGR82BFREE
      @ITZGR82BFREE 4 месяца назад +1

      @@FishQuest Sorry i popped that number off the top of my head. Your number is correct for the melting point of ZINC. I have wrecked a few batches of lead and it doesnt take much zinc to do it. I collect from tire shops around town and these days i keep all the zinc for casting things other than boolits. Thanx

    • @FishQuest
      @FishQuest  4 месяца назад

      @@ITZGR82BFREE right on, thanks again!

  • @dahlusional1
    @dahlusional1 Месяц назад

    What about the zinc weights do those melt down with the lead?

    • @FishQuest
      @FishQuest  Месяц назад

      The zinc has a higher melting temp than the lead so they are easily scooped off with the steel scrap however they can melt and “poison” the lead batch.

  • @tokay999
    @tokay999 Год назад +1

    Where did you buy that mold?

  • @ryanlilly1293
    @ryanlilly1293 7 месяцев назад +1

    What was the pour you used at the end for the sinkers

    • @FishQuest
      @FishQuest  7 месяцев назад +1

      @ryanlilly1293, the pot I used was a Lee Pro 4 20LB, I modified the pot by adding a piece of 3/4” plywood between the base and the back to make it stand tall enough to pour into my big 14 oz sinker molds. I’m currently working on a video that goes over my gear I use and the process of making sinkers.

    • @ryanlilly1293
      @ryanlilly1293 7 месяцев назад

      @@FishQuest sweet thank you

  • @outdoorinterests
    @outdoorinterests Год назад +1

    Have you ever bit onto tss shot, a proper tooth breaker. I have enough pure and alloy lead to last three lifetime's.

    • @FishQuest
      @FishQuest  Год назад

      I mainly find my self hunting grouse in Utah and occasionally a bb slips past me and I catch it on a tooth!

  • @sultanayub4975
    @sultanayub4975 5 месяцев назад +1

    We r working in mine of lead

    • @FishQuest
      @FishQuest  5 месяцев назад

      that's cool, what country?

  • @sultanayub4975
    @sultanayub4975 5 месяцев назад +1

    How can we get earning by lead

    • @FishQuest
      @FishQuest  5 месяцев назад

      I have seen people sell lead ingots on Facebook Marketplace as well as Ebay. There are groups on FB that teach how to process and sell lead. I'd start there.

  • @juliosalas6907
    @juliosalas6907 7 месяцев назад +1

    Use wax to clean the Lead

  • @vansicklejerry
    @vansicklejerry 3 месяца назад

    Wheel weights are crap now. They don't use pure lead mostly anymore. I just bought a bunch from my local junk yard and it don't melt with a lead smelting pot. :( smh

    • @FishQuest
      @FishQuest  3 месяца назад

      The sad truth about used wheel weights is that as the years pass actual lead wheel weights become harder to find. Have you tried going to your local scrap yard to see if they will sell you other forms of scrap lead?

    • @vansicklejerry
      @vansicklejerry 3 месяца назад +1

      @@FishQuest I haven't stopped by there as it's like 30 miles away. I called them 2 days ago and had to leave a message, but they never returned my call. I'll have to call them again next week.

  • @kevinnorthington5324
    @kevinnorthington5324 4 месяца назад

    Trump lost 😂😂😂😅

  • @timgordon1760
    @timgordon1760 7 месяцев назад +2

    GREAT VIDIO