    Best fiberglass tutorial I've seen yet on RUclips, this guy is a good teacher

  • @bradleyplummer5778
    @bradleyplummer5778 2 года назад

    Needing to make panels and such at work. This video has helped a TON for me to create the molds. Plenty of good information within the video! TY!

  • @a11an72
    @a11an72 3 года назад

    Tnx man , these are great videos for amateur diy'ers like me , the endresult on the followup video to this is exactly what im after .... best wishes from Norway

  • @OMEN-TV
    @OMEN-TV 4 года назад

    THANK YOU VERY MUCH FOR THE LESSON! i was searching hours on youtube for a tutorial like yours.But mister i really respect you health came first,please use a mask when working with fiber/polyester.Great video again!

  • @shahrulziman7752
    @shahrulziman7752 2 года назад

    The ultimate teaching video

  • @premnakarmi2580
    @premnakarmi2580 3 года назад

    Thanx for making Small fiberglass mound in detail.but how to clean after using brush plz ?

  • @liamodonnell469
    @liamodonnell469 2 года назад +1

    So well explained Well done

  • @stevew6141
    @stevew6141 2 года назад

    Great video, can ova be used as a barrier between the plug and the gel coat? Thank you

  • @josuedeasisjr2140
    @josuedeasisjr2140 3 года назад +2

    How long before you coat the resin on top of the gelcoat ?

  • @Pushyhog
    @Pushyhog 4 года назад

    try mavcoat release if ya want the best. Part will fall out, Boeing buys it by the 55 gallon barrels.

  • @maqyotvblog
    @maqyotvblog 3 года назад

    very thanks, this tutorial is very clear. i hope others can see this video.

  • @chuckeynewkirk199
    @chuckeynewkirk199 2 года назад

    Good video love the details

  • @sidheshchari154
    @sidheshchari154 11 месяцев назад

    Nice work sir

  • @jernejp7579
    @jernejp7579 5 лет назад

    Hi CFS,
    Like your videos on you tube, very useful and detailed, thank you for your contribution.
    While watching this video I was wondering what is the green base material of, where the model is attached on?

  • @berniestorr5508
    @berniestorr5508 7 лет назад +2

    Hi Paul ,If you use the mirror glaze release wax do you also have to use the spray on PVA release agent befor you gelcoat

    • @garyengland5326
      @garyengland5326 5 лет назад

      No, but using pva gives an extra layer of protection. But, the mould will need wet sanding and buffing, because pva doesn't go on perfectly smooth

  • @ShabirAhmad-oe3dq
    @ShabirAhmad-oe3dq 2 года назад

    Lemineshan mat is the Epoxy resin

  • @glengullickson6538
    @glengullickson6538 Год назад

    Looks like that is all done with polyester(?) Can the same scenario be done with epoxy? Thank you.

  • @AutoFreak10
    @AutoFreak10 3 года назад

    Could I ask how you would recommend making a tunnel for my steering arm to pass through? I had to cut a hole in the fibreglass to allow the steering arm to enter but although not that important as it only goes into a well, I was wanting to make a fibreglass tunnel for it but there is lots of bends and shapes that would be required for the surface part before it enters into the tunnel.

  • @seechurndinesh9710
    @seechurndinesh9710 Год назад

    How many minutes should the gel coat dry to apply the fibres?

  • @glengullickson6538
    @glengullickson6538 Год назад

    Did you let the first gelcoat kick off before applying the second?

  • @61riaz
    @61riaz 4 года назад

    Wow really amazing idea can shared

  • @SkylarkCamperAdventures
    @SkylarkCamperAdventures 3 года назад

    Brilliant tutorial, learnt a lot from that 👍🏻

  • @frankpineda1832
    @frankpineda1832 6 лет назад

    Wow beautiful work 👍

  • @garydeandeery
    @garydeandeery 2 года назад

    I can never get the mix right I only do small mixes and don’t even get 5 mins till it’s going off Say if I do 20 mils do I do 2 drops of catalyst. Coz I’m doing 0.5 in the syringe and don’t have any time to work with it I did 50 mils before with 1 on the catalyst and then it was not going off was sticky still so I went over it with epoxy resin

  • @chamindanissanka1378
    @chamindanissanka1378 3 года назад

    Best job sir,

  • @audiesalminao3635
    @audiesalminao3635 Год назад

    Amazing

  • @chandrashekhardeshmukh4887
    @chandrashekhardeshmukh4887 4 года назад

    which jel coat useing

  • @adamcatlow7496
    @adamcatlow7496 4 года назад

    Would this work with my Europe dinghy

  • @TimPalfrey
    @TimPalfrey Год назад

    Is this guy using polyester resin without a respirator?

  • @গায়েরখবর
    @গায়েরখবর 5 лет назад

    What matarial used can you talk me please please please

  • @rct2
    @rct2 3 года назад

    Great video but can I ask how long between each layer of glass did you leave it?

  • @Rick-tb4so
    @Rick-tb4so 6 лет назад

    Well done......What is the name of the 1st mat you applied to the mold ??

    • @garyengland5326
      @garyengland5326 5 лет назад

      Surface tissue

    • @dantheman321
      @dantheman321 5 лет назад

      @@garyengland5326 do you have to let the surface tissue layer dry before you add chop strand or can you work straight through ? Many thanks in advance

  • @bangsabar3689
    @bangsabar3689 Год назад

    Good👍

  • @bazzarr
    @bazzarr Год назад

    Fiberglass ASMR.

  • @BlackHearthguard
    @BlackHearthguard 7 лет назад

    How would you mold a hull that has a tumblehome in it? Is it possible to do it this way?

    • @johnrutherford8246
      @johnrutherford8246 4 года назад

      If it's a coble shape, you need to make a two piece mold. It's the only way.

  • @sakibian01
    @sakibian01 5 лет назад

    polyester resin?

  • @sunilkumararickattu1845
    @sunilkumararickattu1845 5 лет назад

    Sorry to inform you that did not mentioned what grade fiberglass mate use [first/light weight thjn mat] prior to second lair of 450 csm mat and ratio of MEKP using with. That is very important in a professional manner?

  • @harrydavepagaoa4709
    @harrydavepagaoa4709 6 лет назад

    hello, what if I did not put gelcote, will it work??

  • @patrickhall1532
    @patrickhall1532 8 лет назад

    Looks exactly how i pulled mine out seeing as this is my boat plug😂

  • @simonac688.
    @simonac688. 2 года назад

    wow 👍

  • @suragvs2870
    @suragvs2870 3 года назад

    I am looking fiberglass job any vacancy in your company

  • @doranagedoranage1651
    @doranagedoranage1651 2 года назад

    👌👌❤️

  • @DINHVANTAM-QTRI
    @DINHVANTAM-QTRI 3 года назад

    Hello

  • @michaelrommedahl525
    @michaelrommedahl525 7 лет назад

    Powder- or emulsion- bound Mat...???

    • @garyengland5326
      @garyengland5326 5 лет назад +1

      Emulsion, powder is for epoxy, emulsion is for polyester

  • @mohamadnaeemgurchani5898
    @mohamadnaeemgurchani5898 5 лет назад

    best .thanks

  • @ShabirAhmad-oe3dq
    @ShabirAhmad-oe3dq 2 года назад

    Leminesh polyester resin Epoxy resin

  • @298CRE8
    @298CRE8 7 лет назад

    If your viewing this don't take what he says as gospel and watch other vids this is ok for basic techniques and fibreglassing but not anything else find better vids or research more plenty out there 👍

  • @berniestorr5508
    @berniestorr5508 7 лет назад

    ??