- Видео 108
- Просмотров 2 328 770
BURO's Weld Life
Япония
Добавлен 16 ноя 2017
Mainly transmits practical videos of CO2 semi-automatic welding! This is a support channel for those who are having trouble with welding! I have 20 years of experience in welding and have some skills and knowledge, so I would like to help you in any way I can!
I have 20 years of welding experience and have some skills and knowledge, so I will help you in any way I can!
WES Level 2, Steel Production Management Level 1, Robot Operator, etc.
Experienced 5 national welding technology competitions
7th place in the nation
Started posting on You Tube in earnest on March 27, 2023 and reached 300 subscribers on April 17, 2023!
Reached 400 subscribers on April 25, 2023!
May 5, 2023: 500 subscribers!
May 13th: 600 subscribers!
June 3, 2023: 800 subscribers!
June 22nd: 1000 subscribers!
Thank you to everyone who has registered!
We will continue to do our best to provide you with useful information (^o^)!
Translated with DeepL.com (free version)
I have 20 years of welding experience and have some skills and knowledge, so I will help you in any way I can!
WES Level 2, Steel Production Management Level 1, Robot Operator, etc.
Experienced 5 national welding technology competitions
7th place in the nation
Started posting on You Tube in earnest on March 27, 2023 and reached 300 subscribers on April 17, 2023!
Reached 400 subscribers on April 25, 2023!
May 5, 2023: 500 subscribers!
May 13th: 600 subscribers!
June 3, 2023: 800 subscribers!
June 22nd: 1000 subscribers!
Thank you to everyone who has registered!
We will continue to do our best to provide you with useful information (^o^)!
Translated with DeepL.com (free version)
【横向き溶接】何が良くて何が悪いのか全て分かります
以前出した、工場AW検定鋼製横向きと同じ電気になります。
端部のやり方はこちらの動画より以前の動画を参考にして欲しいです!
カメラがあってやりにくかったので中途半端なやり方でしか出来なかったので!
ノビテック溶接カメラで撮影しているのでかなり鮮明に映っています!何か一つでも参考になれば幸いです!
🔶他の溶接動画
ノビテック溶接カメラで撮影した動画
下向き【完全溶け込み溶接】
ruclips.net/video/gkNLPYxwxXo/видео.html
-----------------------------------------------------------
下向きガウジング動画
ruclips.net/video/YMZhuzNdxdk/видео.html
空調服紹介してます
ruclips.net/video/qWAQ0aS5FhU/видео.html
高性能100V溶接機紹介
ruclips.net/video/OCdstK6Hos4/видео.html
被覆アーク溶接
A-2H
ruclips.net/video/c-56Udb-1iA/видео.html
A-2F
ruclips.net/video/euGIo6V4Gs0/видео.html
ルートギャップなどの専門用語はSA-2Fの動画やブログで解説しています!
ruclips.net/video/fGQ1gM-Z9sU/видео.html
Sfil-FVH曲げ試験ありすみ肉溶接
ruclips.net/video/Y9xqlKNKmMo/видео.htmlsi=MhgLCojOPK1C_Yyq
AW検定代替横向き溶接
rucli...
端部のやり方はこちらの動画より以前の動画を参考にして欲しいです!
カメラがあってやりにくかったので中途半端なやり方でしか出来なかったので!
ノビテック溶接カメラで撮影しているのでかなり鮮明に映っています!何か一つでも参考になれば幸いです!
🔶他の溶接動画
ノビテック溶接カメラで撮影した動画
下向き【完全溶け込み溶接】
ruclips.net/video/gkNLPYxwxXo/видео.html
-----------------------------------------------------------
下向きガウジング動画
ruclips.net/video/YMZhuzNdxdk/видео.html
空調服紹介してます
ruclips.net/video/qWAQ0aS5FhU/видео.html
高性能100V溶接機紹介
ruclips.net/video/OCdstK6Hos4/видео.html
被覆アーク溶接
A-2H
ruclips.net/video/c-56Udb-1iA/видео.html
A-2F
ruclips.net/video/euGIo6V4Gs0/видео.html
ルートギャップなどの専門用語はSA-2Fの動画やブログで解説しています!
ruclips.net/video/fGQ1gM-Z9sU/видео.html
Sfil-FVH曲げ試験ありすみ肉溶接
ruclips.net/video/Y9xqlKNKmMo/видео.htmlsi=MhgLCojOPK1C_Yyq
AW検定代替横向き溶接
rucli...
Просмотров: 3 446
Видео
完全溶け込み溶接(Full penetration welding)1G 下向き溶接
Просмотров 6 тыс.28 дней назад
ノビテック溶接カメラで撮影したものです! 自分もまだ未熟ですが、今回の動画の通り出来ると欠陥は皆無です!欠陥に悩まされている方が少しでも参考になると幸いです! ※3:48の最終層は熱が入っているとアークで狙わなくても溶けると言っていますが!開先が残り過ぎている場合や熱が入っていないと溶けない可能性があるのでご注意を! 🔶他の溶接動画 下向きガウジング動画 ruclips.net/video/YMZhuzNdxdk/видео.html 空調服紹介してます ruclips.net/video/qWAQ0aS5FhU/видео.html 高性能100V溶接機紹介 ruclips.net/video/OCdstK6Hos4/видео.html 被覆アーク溶接 A-2H ruclips.net/video/c-56Udb-1iA/видео.html A-2F ruclips.net/v...
初心者でも簡単!ポータブル発電機の使い方と注意点【溶接DIYも有り】
Просмотров 72028 дней назад
🔶目次 基本機能紹介 1:30〜 【エンジンをかける前にすること】 ⚪ガソリン取り扱いについて 7:36〜 ⚪エンジンオイル取り扱い、入れ方 9:46〜 ⚪バッテリー接続 10:50〜 【発電機を使用後、運搬するには】 11:47〜 【次回の使用が3ヶ月後、一時保管】12:08〜 【長期保管する場合】13:01〜 🛠️メンテナンス 【プラグ清掃】14:37〜 【エンジンオイル交換】16:23〜 【エアフィルター清掃】17:00〜 【ストレーナー清掃】19:45〜 【マフラー清掃】20:02〜 🔥組み立て、溶接 21:35〜 災害時、あなたが使うことになるかもしれません! 発電機の取り扱いは知って損はないです! 最低限取り扱いを知っていれば事故も防げます! メーカーからは、保証期間内であれば無料で部品を再発送し、交換できます。保証期間外の場合は、部品を購入して自分で交換することができま...
Learn from the Welding Gurus! Perfect beads and must-know beginner tips
Просмотров 17 тыс.Месяц назад
こちらの動画に対して誹謗中傷等のアンチコメントを見つけた場合、しかるべき対応をさせて頂きますのでご注意を! YUSEIさん yusei.2022?igsh=NmgzZndsNTQ3ODA2 鳴呼頭(アーヘッドさん) ahhhhead?igsh=Nm82aTR2eXFnajVh 内藤制作所内藤さん welding.2000?igsh=bnBwaTBkd3Fsa293 千葉県パパさん runapapa1124?igsh=MWkzdmRlY2N2MWtwNg 鷹之巣さん takanosu3?igsh=cjlzcmR3eXVnc3cx てらさん plant_weld?igsh=MTJ4eXg5YzdhaHdndA ティックトッ...
Don't miss out on the craftsmanship! Do not blink
Просмотров 26 тыс.2 месяца назад
僕が尊敬する凄い方達です! 中にはSNSに投稿されていない貴重な画像もあります! ご協力頂きましてありがとうございました! こちらの動画に対して誹謗中傷等のアンチコメントを見つけた場合、しかるべき対応をさせて頂きますのでご注意を! 🔶インスタグラム 1人目 兵庫県金本さん welder358t welder358t?igsh=Z2F4MjBhc3hjdWpl 2人目 沖縄県Shoさん Sho_93_ sho_93_?igsh=ZHYyc3Nna3hsd21s 3人目 とある地区のようせつ君さん kobee51t kobee51t?igsh=emoxcHZienJvdGtk 4人目 福岡県コバさん kb_weld kb_weld?igsh=Zmo3OW9wa3ViaWEz 5...
Corner welding class with 20 years of welding experience
Просмотров 6 тыс.4 месяца назад
Corner welding class with 20 years of welding experience
Performance Beyond Price] EENOUR Semi-Automatic Welding MIG120L Complete Guide
Просмотров 45 тыс.4 месяца назад
Performance Beyond Price] EENOUR Semi-Automatic Welding MIG120L Complete Guide
Explanation of how to fill in the gaps between tabs and how to shave them successfully.
Просмотров 51 тыс.5 месяцев назад
Explanation of how to fill in the gaps between tabs and how to shave them successfully.
(SMAW) Standing facing, bending also done, repair welding method explained.
Просмотров 12 тыс.5 месяцев назад
(SMAW) Standing facing, bending also done, repair welding method explained.
A must-see for welding beginners [Fillet vertical welding]
Просмотров 12 тыс.7 месяцев назад
A must-see for welding beginners [Fillet vertical welding]
Improvement of bumpy welding] Explanation of vertical welding
Просмотров 9 тыс.7 месяцев назад
Improvement of bumpy welding] Explanation of vertical welding
32mm Welding know-how assuming truss beams
Просмотров 9 тыс.7 месяцев назад
32mm Welding know-how assuming truss beams
Highly difficult stand-up welding explanation
Просмотров 11 тыс.8 месяцев назад
Highly difficult stand-up welding explanation
Welding techniques of skilled welders open to the public
Просмотров 19 тыс.8 месяцев назад
Welding techniques of skilled welders open to the public
I will show you a special technique that utilizes the functions of the welding machine.
Просмотров 17 тыс.9 месяцев назад
I will show you a special technique that utilizes the functions of the welding machine.
19mm vertical welding know-how with flux-cored wire
Просмотров 28 тыс.10 месяцев назад
19mm vertical welding know-how with flux-cored wire
I made minions using a metalworking technique that no one knew about.
Просмотров 3,1 тыс.10 месяцев назад
I made minions using a metalworking technique that no one knew about.
Good and bad welding of shielded arc downward welding (JIS test) is also explained.
Просмотров 26 тыс.11 месяцев назад
Good and bad welding of shielded arc downward welding (JIS test) is also explained.
Introduction of corner welding method that produces downward, vertical, and horizontal strength
Просмотров 15 тыс.11 месяцев назад
Introduction of corner welding method that produces downward, vertical, and horizontal strength
2G horizontal welding] technique that no one teaches you is revealed.
Просмотров 128 тыс.Год назад
2G horizontal welding] technique that no one teaches you is revealed.
Japan's high degree of difficulty qualification! Full penetration welding explanation
Просмотров 23 тыс.Год назад
Japan's high degree of difficulty qualification! Full penetration welding explanation
溶接する前にカメラより赤いレーザー光見たいの出ているのですが、開先深さとかの測量をおこなっているのですか?
あの赤い部分が映像に映る場所なんですよ😊目印みたいな感じだと思います😊
教えてくださる先輩がいて幸せだなぁ~と思いました😢
😂😂😂
ワイヤーは?YM?
YM-50です!
映像が超鮮明で本当に感謝です。 アークとプールの先端がよく見えるので、また自分の溶接に活かします! いつもありがとうございます。
良かったです🥹 これからも投稿頑張ります💪💪
なんか このカメラ画像 わかりにくいな 普段見た事ない画だから 当然か
人によって分かりにくいって方います🤣
9cbで、やってくれ😊
9cbってなんですか??
@@buroch クロム系の溶接棒✌️
溶接とは強度もさる事ながらボルトなどの部品をはぶきメリットが多い 以前製缶工やっている時先輩から3ヶ月やって出来なければやめた方が良いと言われ現在に至るが動画の通りこれが本当の溶接だと言うことがわかるJIS規格の合格ラインをもっとあげて良いと思う
3ヶ月で見切りつけるのもなかなかですね🥹 でも確かに飲み込み早い人は3ヶ月あればビード真っ直ぐ走るくらい出来ちゃいますよね! JISの合格基準は大分甘くなってきてます😂
プロの説明は信頼できますね。
ありがとうございます🙇♂🙇♂🙇♂
ぶっちゃけ溶接上手い人、下手な人いると思いますが、何が原因で上手い下手が決まると思います? 熟練者の先輩にしっかり指導してもらえたかどうかでしょうか?
熟練者の教えるのが上手い人の指導は大事ですよね! 教えて貰っても言ってることが理解出来ないことは自分で考えてやるしかないですが やっぱり本人のやる気ですかね! 下手な人は「もっと上手くなりたい」という気持ちを持ち続けられていない気がします! それと、上手くならない人は自分に甘い人が多いです!他責な人多いですしね。 飲み込み早い、遅いは個人差はあります 後は、仕事が暇な時にアーク出さないで遊んでる(笑)😂
すごい綺麗っすね〜! ガスはCO2ですか?
まだまだですがありがとうございます🙏 CO2ですよ😊
腕が良いですよね。なかなか慣れるまではここまで行けませんよね、弾くと抜ける感覚勉強なりました。
20年やってますから💪 そうですね😢 コツさえ分かればなんですけどね!
ヤバすぎますな😂
上手い人なんか5万といると聞きますが、ほんとにいそうです🥹🥹
みなさんは、超音波検査の手直しできますか?半自動の難しさは手直しだと思います
@@gantz1504 半自動普段から使っている方なら手直し出来る人達だと思います😀
スパッタ全然ないですね! ワイヤー何使ってるんですか?
フラックスのFCM-1Fですよ!
本電流のみで回す場合、アーク発生は角で行いますか? 動画だとノズルでワイヤー先が隠れちゃってて....
@@games-tr3zj あ〜😂すみません😂 角の辺で問題ないと思います!
ありがとうございます! これからも投稿頑張ってください 毎回数十回リピートして勉強させてもらってます。
@@games-tr3zj ありがとうございます🥹🥹 これからも投稿頑張ります(^^)
自分はスパッタ付着防止剤はノズル外してウェルパー等で挟んでノズルだけ突っ込んでますw チップの先に防止剤が絡まって玉になったり、オリフィスの穴に垂れるのが嫌で....
@@games-tr3zj やり方結構人それぞれですよね😀
もはや横向きw
本当それです(笑)🤣
初溶接検定を受けてきました! 下記内容についてご教示いただけますでしょうか。 1層目を180A、後進法で行なったのですが、半分を過ぎたあたりから「ポンっポンっ」のような「パンパンっ」のような音が変になりビードを見ても後半からはビードが少し凸っぽくなってしまいました。 なぜこのようなことが起こるのでしょうか? またそれはやはり裏曲げ試験に影響してきますか?
@@sushi-p9e 電圧が微妙にあってなかったんじゃないですかね?🤔 電気合ってないと曲げにも影響は出ます! 低い電流だと特にですね!
是非四つ割りで揃えてみてください✨
後退方で溶接する時に開先の溶けが見えづらいのは重々承知しているのですが、溶接中、意識して見ている箇所やコツなどはありますか?
こちらの動画内容もそうなんですが、僕が出している下向き溶接の動画に意識している箇所や、コツを全て話しています😊 何か分からないことがあればなんでも聞いて下さい!画質は悪いですが、SA-3Fの動画で基本的なことは多く話しています😊
第三弾載せて欲しいです😂
12月か来年度には!🫡🫡
溶接って手直しが一番つらくて大変!
本当ですよね😂
うま過ぎる!
ありがとうございます🥹🥹
電気設定知りたいほど綺麗(教えてください)
@@ピンスケ-z7g 確か330Aくらいでやったような🤔電圧は感覚で合わせてるので忘れてしまいました😂
@@buroch ありがとうございます!電圧は電流よりは高いですよね??
回しのときL字に回してるんですけどそれってダメなんですかね?みんなおしりみたいに回してるんですけど自分はストレートで持ってった後L字にクレーターで作ってからストレート後退法で溶接してます。
@@ピンスケ-z7g 駄目ではないと思います! 稀に回し方お尻みたいに真ん中で繋げるの駄目な時ありました!
@@buroch 臨機応変って感じですね😁
「道具にも愛を」ってよく 測量の教員に言われてました。
@@血飲み子 良いことですね!😊自分でお金出してないから雑になるんだと思います😅
本当にありがとうございます!
@@user-pq3pt2t こちらこそ見て頂いてありがとうございます😊
感覚的にVビードは緊張感があるから建築物とかは抜群に合いそう。 にしても完璧な溶接、素晴らしいです。
@@三識 コメントありがとうございます🙇♂ Vビード出すの面白いです🥹 まだまだですがありがとうございます🙇♂
buroさん全国大会頑張れー🔥
あと2週間しか練習出来ないので本番までには完璧な状態で迎えたいと思います🔥ありがとうございます🥹🥹
変態w
@@momochanmomochan7997 否定はしません🤣🤣
スーパーきれい
@@こーすけ-n4s まだまだですがありがとうございます🙇♂🙇♂
溶接を始めて物作りにハマっているのですが、溶接は良くても鋼材の向きとか組み方とかが全然理解できてません。例えばチャンネルの歯を内側にむけてつけるとかそういった知識はどの本で身につければいいですか?またよろしければ動画などで紹介してほしいです。L型アングルを内向きではなく外向きで柱として使う、チャンネルの歯を外側に向けて柱として使うとどんな事になるとか
@@Sfahjcujeyheicknci5638 www.tiktok.com/@rivi_h30?_t=8qJira4FC5a&_r=1この方の結構勉強になると思いますよ! 僕は設計に関してはそんなに詳しくはないです😂 基本鉄骨に関してはJASS6の教科書を見ると勉強になるとは思います!
@@buroch ありがとうございます
@@buroch 3点質問があるのですが、ガス抜き穴を開ける際は何ミリの穴をあけますか? 2点目は穴を開け終わって作業の終わりに穴を埋める際は溶接のみで穴を埋めても大丈夫なのでしょうか? 3点目は柱と板を一緒に溶接する際はフル溶接が基本ですか?角をチョコチョコと数点溶接するのはマズイでしょうか?
@@Sfahjcujeyheicknci5638 コラムの柱の場合はガス抜きの穴は確か19ミリか21ミリあけてます! 柱の天辺のダイアフラム中央にあけた穴は物件で色々ありますが雨が中に入らないように溶接で穴埋めする場合ありますよ! 柱と板のフル溶接はメッキでは基本です! その際、設計の段階でコラムのR部分に溶接がかからないように考えて貰わないといけないですね!NGなので! 分かっていない設計屋さんたまにいます😂 ペンキの場合は5分穴は基本全周溶接、四分穴は全周ではなくショートビードにならないように40〜50ミリ盛ります!会社によってやり方は違いますね! 基本的にはどうしようもない場合を除いて小さいビードをチョコチョコ盛るのはショートビードになるので良くはないです! コラムの柱の角埋めを下向きで人の手でやるとショートビードの塊と言う検査員もいます😂
@@buroch 何も知りませんでした、板と角パイプ言われるように溶接して板が曲がった場合はどうされてますか?
綺麗なビードって憧れても 仕事内容と、環境、使ってるワイヤー すべてが一致してることはまずないから あんまり追求しすぎないようにしないと 心折れて溶接やりたく なくなるから、理想ばかり追いかけると結構躓く事多い でも、憧れちゃうなぁ
@@smartmoy2462 いろんな方いらっしゃいますよね🥹
いいねー👍🇧🇷🇯🇵👊
@@shohachi5471 ありがとうございます🥹
すばらしい、それいじようのことばがでない👍🇧🇷🇯🇵👊
@@shohachi5471 第三段もやりますので、よろしくお願いします😊
この変態め! どうせやってる間は時間忘れる廃人だろ? すばらしいわ!!
@@momochanmomochan7997 まさにそうです🤣🤣ありがとうございます🤣
大会等の記録教えなさいよ!この変態!w
そんな掃除の仕方してました。それで混合ガスなので、すぐブロー入ってました
結構知らない人いるんではないかと思いまして!😢
いや久しぶりにめちゃくちゃうまいなこの人っておもった。通りすがりで色々見入ってコメかきこいました🙏 俺は今年溶接歴18年 あーまだまだこの仕事面白いなって思えました。あざす! すげっす!
嬉しいお言葉!!🥹ありがとうございます🙇♂ 何気ない溶接でも見方を変えればどこまでも追求出来る仕事なのでとてもやりがいを感じます! まだまだですがこれからも精進していきます😊ご安全に🫡
Good Camera 👏👏👏
@@S0oP0 Thank you📷📷📷📷
溶接汚い😡💨
@@user-xp8hv8io6t すみません😂頑張ります😂
下手くそ
あのぉ~BGMが頭の中で無限ループされるぅ~
曲気に入って貰えて良かったです🤣🤣🤣 たまたまオススメにあったので(笑)
うまっ!スパッタもほぼ無し!素晴らしい👍
@@まるお-e3q ありがたいお言葉!! まだまだ精進します😊
電圧合ってなかったらワイヤーが叩く事が多いねブラック企業になると不具合しか無い溶接機で上手い事やってる人がほめられる😂会社は治そうとしないしょぼすぎ状態になるからそんなとこには決して就職しない事をお勧めする
@@butanizinkennai まさにそうですね! 会社によって全然違いますよね😂気をつけます🥹
あーぁ練習あるのみだね👍
やってみたんですか?練習あるのみだと思います🫡
A高い方が滑らかに仕上がるのにJISの規定Aは低すぎるの何で?
板厚と使用ワイヤーの特性もあると思いますよ😀JISは裏当て金が六ミリなのもありますし、仕上げ電流高い人もいると思います!
コメント失礼致します。 使用されているのは交流溶接機でしょうか?
交流になります!僕の知る限り試験会場も交流なので!
@@buroch ありがとうございます🙇♂️
すご!!
ありがとうございます🙏🙏🙏
うま
ありがとうございます🥹🥹