- Видео 19
- Просмотров 316 934
J and L Metals
Добавлен 10 апр 2021
Gold silver copper refining and casting! Platinum palladium and Rhodium from Catalytic Converters!
Rhodium, Palladium and Platinum from Catalytic Converters Part 2
This is the second part of my video where I attempted to separate the platinum group metals but ended up melting them all together.
Просмотров: 14 138
Видео
Rhodium, Palladium and Platinum from Catalytic Converters Part 1
Просмотров 17 тыс.Год назад
This is the first part of me extracting platinum group metals off of catalytic converters at home using acid and aluminum.
Silver Recovery from Gold Refining Waste
Просмотров 8 тыс.Год назад
I am recovering silver from all my waste leftover from my last gold refining video. I then melt them down into a nice bar and Viking coins.
Scrap Gold Refining into Half Viking Coin
Просмотров 777Год назад
Scrap Gold Refining into Half Viking Coin
Silver Copper and Aluminum Viking Coin Casting
Просмотров 509Год назад
This is a video of me casting Viking coins out of copper silver and aluminum in my garage. 
Viking Coin Casting in Copper
Просмотров 382Год назад
This is me for the first time attempting to forge a Viking coin in copper from a new mold.
Gold Panning, Gold Pay Dirt
Просмотров 512Год назад
This is a video of my wife and I doing a gold painting review. 
Precious Metals From an Amazon Kindle
Просмотров 808Год назад
Recovering precious metals from a Amazon Kindle.
Louisiana Gumbo
Просмотров 211Год назад
This is a recipe that shows you how to make a smoky version of traditional Louisiana gumbo.
Gold Recovery from Electronic scrap Part 4 (Military Grade Pins)
Просмотров 2,5 тыс.Год назад
I extract gold from military grade gold plated pins and refine some silver through the process.
Gold Recovery from Electronic Scrap Part 3 (CPU’s with Silver Recovery)
Просмотров 2,9 тыс.2 года назад
This is me in my garage recovering gold and silver from scrap CPU’s.
Gold Recovery from Electronic Scrap Part 2 (Ram Sticks)
Просмотров 2,4 тыс.2 года назад
This is me in my backyard and garage salvaging gold from trimmed ram sticks!
Gold Recovery from Electronic Scrap Part 1 (Circuit Ends)
Просмотров 4,5 тыс.2 года назад
This is a video of me attempting to recover gold from scrap circuit end and a SIM card reel.
Platinum, Palladium, AND RHODIUM from Catalytic Converters!
Просмотров 194 тыс.2 года назад
This is the entire process from start to finish recovering platinum, palladium, and rhodium from nine catalytic converters at home. This is an extremely dangerous process. Hope you enjoy.
Gold from Computer Parts / scrap
Просмотров 2,3 тыс.2 года назад
I am extracting gold from scrap computer parts such as CPU’s, and ram sticks using aqua regia.
Bunk video
where you get you scraps from
Mostly EBay
Ban viế lên từng loại hóa chất loại nào vào chước noại lào vào sau quy trình từ đấu đến núc song hộ mình có được o vì mình o hiểu ban nói csi rì cả
Bạn làm một hài làm ba li um từ bắt đâu hộ mình có đươc o cho mình sin
ممكن سؤال لو سمحت انا عايز اعرف إسم المواد عشان الذهب الابيض ايريديوم إسم الماء الملكي عشان ايريديوم الذهب الابيض واسم المواد الكيمياء عشان الترسيب ايريديوم وشكراا جداا
Dam dangerous but cool to watch funny thing as you poured the bleach in the barrel I'm turning my head away from my phone as if I'm gonna smell those gases..lmao Cool
Very cool video. I always wondered why the theft of catalytic converters are on the rise nowadays. Cool video the science behind it all. Be safe.
hey man I need to contact you I have rhodium how is your process pls dm
Wtf dude you're taking a lot of unnecessary risks.
I would like to know the ingredients that I need to do this process from start to finish sir
I just got into your Channel and Watched your Videos. Just Realized you haven’t Uploaded in over a year and a Half Hope All is Well And You Start to Upload Again. It’s May 2024 I’m Commenting Last Vid Posted was April 2023….!!??
So I’m in the military and have been deployed. I will start posting videos again around October 👍
Fill like I came into the middle here.what is solution and where did gold and silver come from
The adding of the acid after the aluminum only dissolves your PGMs again, it doesn't create or drop more PGMs
Using thicker aluminum will make your PGMs fall in larger clumps. Making settling and separating it 100xs easier
Awesome. Thanks for the advice!
Always keep your material damp as the majority of your valuable materials are light and will float away
Not worth a bollox
Thank you for your video, from Chile South América 🎉
Çok güzel olmuş. Silver . Sadece . Sodyum klorür ile . Tuzlu su ile bakır dan ayristiriliyor biliyor dum . Oysa . Cuper boru larla silver çok güzel çöktü teşekkürler
Çok güzel olmuş. Silver . Sadece . Sodyum klorür ile . Tuzlu su ile bakır dan ayristiriliyor biliyor dum . Oysa . Cuper boru larla silver çok güzel çöktü teşekkürler
❤❤❤
Hi bud you used way way to much nitric acid in that lot and then you had to denox it to hell and back try something called incremental doses of nitric view mills at a time when reaction stop put few mills more then you won’t waste nitric acid and then you won’t have to denox to the moon and back watch a fella called ewaste recycler he never ever needs to denox ??????
Hi bud you should have a catch container under your heater so that if you do get a boil over you don’t lose all your gold or silver and you need a light in your hud it’s dark and not easy to see good
Hey there you did an awesome job and I appreciate your efforts.
Where did you get your glass ware??
Thank you
Love the safety sandals
Great video, thanks.
Hello sir.... I'm from Indonesian, Im processing precious metals from natural resources (stone, soil, sand, mud etc.)
I'm from Indonesia, processing precious metals from natural resources (stone, soil, sand, mud etc.)
Did you end up getting platinosis? Guess you might not know for a while.
Have you heard of a full face respirator and pants? Stupid redneck.
Just for everybody paying attention. That magenta facemask he is wearing is for microscopic spores. He will need a black filter for dangerous gases. Can you find the black filter at military surplus stores. They contain charcoal.
Great job and a very interesting video.
Put your solution under pressure and it will speed up the settling process
Good morning, what acidity is recommended for the best reaction,,,,,,,,Buongiorno, che acidità è consigliata per la reazione migliore
PCB gold plating is somewhere around 30 microinches thick...if I did the math right you'd need about 3000 square inches of plated surface to get 1ozt of gold from it. I gotta wonder if the copper would be worth more.
Can cooper wire be used to get the silver out?
The inside of those copper pipes will contain silver
I'm so fascinated with chemistry that's is fun and can make some money from old copper pipes
Whatever that cloud was in your original solution ended up in your silver. My guess is AgCl. Settle it out and decant if it won't clear up with Nitric. No additional HCl as silver chloride isn't soluble and the silver needs to be in solution for cementing to work. Once you've got it clear, *then* do the drop and your dropped silver will be fairly pure after wash. If you want more pure than that, you'll need to involve electrolysis (silver cell). Same applies for copper, except you can acidify copper solutions with HCl since CuCl2 is soluble. If you're *into* electrolysis, copper is easy to recover if the heavier metals are gone first. Using a special type of electrolysis (electrowinning), where a carbon rod serves as the posode, the solution is "driven clean" and all of the copper is deposited out on the cathode for harvest. Low and slow, nice clean take. You can do this with silver as well but slow is key if copper is present. It will also want to go to the cathode with the silver but if the power is set up right, it can still separate them. With copper it can go quicker generally speaking. The metals "above" hydrogen will tend to take higher voltages to come out, so careful selection for the target metal is still useful, but in general hydrogen will be evolved preferentially from solution so many of them will stay in solution. EW is fun to mess with. TLDR; Either way you only want to drop/run in clear solutions or you're somewhat wasting your time. I'd acidify if there's any question, and let it that starting solution settle, decant it and then cement the silver. Filter off the silver, settle solution if needed (or acidify with a little heat, should only be silver metal in suspension now), and electrowin the copper out. If the voltage and current limits are set appropriately, you will have copper plating/crystal growth on the negode and all the metals above hydrogen in solution.
I use a medium grade filter to filter my silver nitrate solution and it is blue a crystal clear. I make sure there is some unreacted silver left or add some sterling silver to make sure the nitric acid is consumed. I use copper pipes and wash out the center of the pipe. Works well for me.
No way?
SUPER 👍👍👍
Dear friend you have a lot of experience in mineralogy I have learned a lot from you long time no new video from you waiting for your video I want to know if there is gold and palladium Precipitate from ferrous sulfate May be
HOWDID YOU GET THEGOLD OUT FIRST
If you're worried about pressure in the barrel, you need a simple airlock. Unless that cap is a very loose fit, it can easily get stuck, and a with barrels that size, it doesn't take that much pressure to make them burst.
Sir I got some metals from some ground mineralized stone by Aqua Regia it has gold along with PGM group metals and again Aqua Regia to make the gold pure it left some amount which Also not dissolving in Aqua Regia could they be iridium?
thank you
You woke up the hand-wringing Karens from under their rocks-pretending to care about your safety but just wanting attention
I see a lot of people use those "bent to broken" copper pipes to pull silver out. But remember, the solution reacts with BOTH sides of the pipe, outside and inside. The precipitated silver falls off of the outside of the pipe, but when it falls off of the inside of the pipes, it can get trapped in the pinched off ends. I usually bend to break the pipe, then take a hammer to the pinched ends to open them up a little so the precipitated silver on the inside of the pipes will fall out.
Dear friend to get Palladium if formic acid is not available, can you use hydrochloric acid instead?