    @MissMilly1987 3 месяца назад

    late to the party but I just did a copper plate class on the weekend and we used asphalt as stop out. It was to stinky and took ages to dry.

  • @overlordofthepies
    @overlordofthepies Год назад

    Very clearly explained, thank you!

  • @robertb3842
    @robertb3842 8 месяцев назад

    Great tutorial, thanks!

  • @MGhv2by
    @MGhv2by 3 месяца назад

    What is mordant mix with gum arabic?

  • @digitalbrayer
    @digitalbrayer Год назад

    Hi there I enjoyed watching your video. Good to know about pros of use. of metallic spray for aquatint (droplets etc). I am wondering if you find that your spit bit mordant (using peroxide etc). performs better than the ferric chloride mordant??