  • @pearlettoi2046
    @pearlettoi2046 2 года назад +4

    The best video on lime plaster I have watched. Thanks for the video

  • @HollywoodCreeper
    @HollywoodCreeper 3 года назад +1

    It looks so good, especially when you are putting it on above that window.

  • @rameshkhanna1331
    @rameshkhanna1331 3 года назад +3

    Very nice information . there are very few people like you . God bless long life to you

  • @jb_90265
    @jb_90265 3 года назад +5

    love seeing the natural lime plaster ... great health benefits when done on the interior. the mesh is perfect for outside. ( for inside it's best to use an adhesive .. like larson's plaster weld .. its pink so you can really see the coverage well ). .. you can do plaster over wood lathe, metal mesh, or gypsum OR magensium oxide board . excellent choice because its very flexible and self healing. thanks for the video !

  • @ltkhongsai5827
    @ltkhongsai5827 4 года назад +2

    Very informative

  • @Plasterer1
    @Plasterer1 3 года назад +2

    Good job 👍

  • @kshitijvermacms
    @kshitijvermacms 3 года назад +1

    nice work

  • @colonelbeatson6027
    @colonelbeatson6027 3 года назад +3

    my dad and i use lime render for patch up work and straw bale work we use brighton cement hydrated lime. stay safe from australia.

  • @dkaloupis75
    @dkaloupis75 3 года назад +2

    Dear sir. You got my subs and thumbs but most important my total respect. Thank you so much for the lessons.

  • @EastyUK
    @EastyUK 3 года назад +3

    Great video mate, there is a lot of information where people don't differentiate between hydraulic and hydrated lime. So great you told us which you were using, I wish we could get hydraulic lime (NHL) in the US, but it's pricey.

  • @garyweber6413
    @garyweber6413 3 года назад +2

    Thanks for teaching us.Im going to try it.

  • @winesap2
    @winesap2 3 года назад +3

    Do you do the process of "knocking up" where the sand and given amount of lime putty are beaten until the calcium binds to the sand? It starts out pretty dry but after the process of beating it for 20-30 minutes, if done by hand, will become more workable. You can also do it with a mortar mixer. You do this instead of adding water to get the right consistency. This is the traditional process apparently and will make a stronger plaster. Adding water can make it weaker and the process of knocking up will make the chemical process go better and bind better.

  • @PanzerBuyer
    @PanzerBuyer 4 года назад +1

    Great job and thanks for sharing! Can you/should you, paint the finished surface and with what type of paint? There are many types of concrete color dyes, that might be an option.

  • @prasadboddupalli
    @prasadboddupalli 3 года назад +4

    Hi, for indoor lime plastering, does one usually apply another layer of pure lime putty on top of lime plaster ? If so, is it for a smoother finish or for better durability or both ?

    • @HollywoodCreeper
      @HollywoodCreeper 3 года назад

      Good question. It would be great if somebody who knows what they are talking about answered it. I thought someone would just apply 1 layer inside or outside. It seems like the second layer would not have enough to grab a hold of even with that scratch.

  • @malik51973
    @malik51973 Год назад

    Gud job,,what is the curing of lime plastering?it is curing like cement plaster that wetting after applying plastering two or three days or lime plaster no need wetting??

  • @stefanharling4614
    @stefanharling4614 3 года назад

    Can you put lime plaster onto a painted drywall? I’m looking to use a limewash finish but I need to plaster over an existing painted wall for the limewash to stick

    • @craigslitzer4857
      @craigslitzer4857 3 года назад

      Just guessing here, but I'd say no. I think drywall and plaster are mutually exclusive. It's probably one or the other, not both at the same time. Again, just a guess.

  • @ernievonvutenhauger7207
    @ernievonvutenhauger7207 4 года назад +1

    Could this plaster be used for interior solid brick walls? Thanks for making this video. Finding proper information on hydrated lime is very difficult to find.

    • @off-gridhomesteading7269
      @off-gridhomesteading7269  4 года назад +1

      Not sure
      I seem to remember reading that type s is the type to get. Wish I knew the difference between them
      I used hydrated lime from a feed store.
      It was the only kind I could find locally

    • @jb_90265
      @jb_90265 3 года назад

      @@off-gridhomesteading7269 usheritage.com/plaster-stucco/

    • @corindoyle
      @corindoyle 3 года назад +1

      @@off-gridhomesteading7269 hydrated is partially slaked quicklime that you can slake with water to putty, in 24 hours, its less reactive so therefore safer to use. Quicklime is for hot mixes. Putty is made from quick or hydrated. NHL is completely different and can't be slaked to a putty.

  • @TimKollat
    @TimKollat 3 года назад

    Isnt it much stronger if you also add cement to the mix? All the stucco/plaster Mexicans in AZ all use a cement based plaster with lime added. Ive never seen any stucco/plaster crew ever use just lime/sand. Seems like it would be far less durable?

  • @WallaceRoseVincent
    @WallaceRoseVincent 4 года назад

    Can you use S Lime for lime plaster? S Lime is commonly found t home depot? Would it require a few days of water absorption too?

  • @saschaceleste9841
    @saschaceleste9841 4 года назад +3

    Can you use this lime plaster formula on a stone fireplace?

    • @off-gridhomesteading7269
      @off-gridhomesteading7269  4 года назад +2

      Good question.

    • @edjackson3663
      @edjackson3663 4 года назад +1

      Yes I have used it on fireplace surrounds before (brick). The problem is that the soot will stain the lime plaster and any sooty surface that you plaster over will start to stain through as the building material breath👍🏼

    • @edjackson3663
      @edjackson3663 4 года назад +1

      And the stone must have a key for the plaster to adhere to

  • @LolitasGarden
    @LolitasGarden 3 года назад

    How did you source your bags of lime?

    • @Jojojamjar
      @Jojojamjar 3 года назад

      any hardware store or garden center. look for "hydrated lime" its the same stuff people put on their garden soil to correct soil pH. Its usually rather cheap. where I live 20kg (44pounds) costs 12$

  • @Jim-K-Baker
    @Jim-K-Baker 3 года назад

    How is it holding up to the weather?

  • @scottwhite685
    @scottwhite685 Год назад

    How does it ever cure on the wall, when it can sit in water for 2 years and still be workable?

  • @titugupta7412
    @titugupta7412 4 года назад +1

    Lime motor bnava lime pani tank katel divas rakhvu.

    • @Sudhakar2310
      @Sudhakar2310 4 года назад

      Minimum 1 week. 1 mahina rakha to best hai

  • @anonoyingmuck8071
    @anonoyingmuck8071 3 года назад +1

    Cannot stress the importance of eyewear and protective equipment as lime will burn the body. Looking at the tennis shoes, I've known of young apprentices getting lime burns on their toes due to this practice when the shoes get wet.

  • @corindoyle
    @corindoyle 3 года назад +2

    Goat hair not plastic fibres. Don't use it with metal either its a strong alkaline.

  • @eagleeye182
    @eagleeye182 3 года назад +3

    It`s extremely important to wear safety gloves and glasses. I even use a plastic shield and safety glasses together. As the saying goes - better safe and sorry.

  • @averageguy7641
    @averageguy7641 3 года назад

    Your beard had me fooled
    Thought u we're gonna be a good plasterer😂

  • @MarkMisterMr.Hamaguchi
    @MarkMisterMr.Hamaguchi 3 года назад

    You don’t need to scratch if lime on lime.

  • @Rubinpa
    @Rubinpa 3 года назад +1

    Too much lime, i would have used more sand.....like 5 to 6 parts to 1 of sand.

  • @grassabrutta
    @grassabrutta 4 года назад

    metal mesh is just junk

    • @anonoyingmuck8071
      @anonoyingmuck8071 3 года назад +1

      What do you suggest other than galvanized 16 gauge expanded metal lath at the exterior? perhaps 17 gauge 1 1/2 inch stucco netting?

    • @TRM1294
      @TRM1294 3 года назад +1

      and you recommend?

    • @corindoyle
      @corindoyle 3 года назад +2

      @@TRM1294 wooden laths or fibre glass mesh if absolutely you must. Metal and strong alkalines like lime do not mix.