  • We recorded the installation of some liners using liquid Nitrogen to shrink the parts before fitting.

Комментарии • 8

  • @abdoucherti3369
    @abdoucherti3369 2 года назад

    That's a scary scene of a shricked bush in the air for 10 sec, good job though it went in

  • @faridmahomed3339
    @faridmahomed3339 7 лет назад +2

    If a want to remove the bushing what should I do????

    • @KarthikKarthik-xk5bh
      @KarthikKarthik-xk5bh 5 лет назад

      This is also my doubt

    • @utekarakshayinfo3597
      @utekarakshayinfo3597 4 года назад

      Farid mahomed how meny time are material in a naitrogan

    • @glenquagmire4232
      @glenquagmire4232 3 года назад +1

      Heat the outside diameter of bushing housing

    • @rafisshakirov5651
      @rafisshakirov5651 2 года назад

      @@glenquagmire4232 do you usually use the heat induction or directly flame ?

    • @QuanDiz
      @QuanDiz 6 месяцев назад

      @@rafisshakirov5651 direct flame. Have 2 guy torching it evenly and one guy with a temperature gun to make sure everything is heated evenly and it will fallout if you do it correctly…missing your mark will mean you need to cool down to do it all over again.