Thanks Chris you helped me way more than the bigger vids out there just saying to stop adding heat. Thanks for the arc length explanation and showing how to set up a gas lens attachment and #12 cup. Bug help.
Finally someone that shows me some things to check as to why I’m getting the grey, was confusing me as it was only happening when using filler wire, guess was prob a combination of a few things
What was your stick out length ? Can you show some gas lens profile shots of you running at .01 to .02 arch length ? What was your CFH ? Pre-flow ? Post-flow ? What is the best grind for this weld metal thickness ?
hello am in Australia.. Have a job that has a lot of steel flooring around job site. Laydown of electode a pain. Using a modern small inverter stick welder. Q) anywhere in USA / your company sell a stick electrode holder with ON OFF switch. ? Have never seem one. Only one on www is one for 12 v vehicle welders it seems. Seems a no brainer to have the option? any info appreciated. Has to deal with wide range amps no doubt.
Thanks Chris you helped me way more than the bigger vids out there just saying to stop adding heat. Thanks for the arc length explanation and showing how to set up a gas lens attachment and #12 cup. Bug help.
Excellent demonstration as always guys.
Chris. Best stainless vid on the tube.
Fabulous lecture. One of the best(probably the best) lectures on stainless steel welding for beginners/novices. Thank you
Thank you! This have been the most helpful video I've seen so far, in Tig welding.
Chris is the MAN!!!!!!
Finally someone that shows me some things to check as to why I’m getting the grey, was confusing me as it was only happening when using filler wire, guess was prob a combination of a few things
Super clear! Thanks a lot!!!
Thanks for this video, wish I'd seen this sooner
Great! I learned something today thanks to you! I definitely need to keep my arc length shorter
Good explanation.
Hi Chris is Cuco996 Congratulations now you’re sharing knowledge good to learn from a celebrity. Yesterday I bought my first Tig 😎😎😎
What movies is he in?
Congrats on your first TIG
I always run a gas lens. And go higher amps than i need with foot pedal variance to control my heat.
What was your stick out length ? Can you show some gas lens profile shots of you running at .01 to .02 arch length ? What was your CFH ? Pre-flow ? Post-flow ? What is the best grind for this weld metal thickness ?
would tig Al benefit with gas as well?
I would have like to seen the back side of the last weld.
What about gas flow vs cup size, etc?
ye yes yes...great stuff
thank you
Thanks for adding subs in Spanish
So you use both insulators with a gas lens? Where'd you find this guy, Everlast?
hello am in Australia.. Have a job that has a lot of steel flooring around job site. Laydown of electode a pain. Using a modern small inverter stick welder. Q) anywhere in USA / your company sell a stick electrode holder with ON OFF switch. ? Have never seem one. Only one on www is one for 12 v vehicle welders it seems. Seems a no brainer to have the option? any info appreciated. Has to deal with wide range amps no doubt.
Why would you Need a switch for Stick welding?
Excelente
Deben hacer la traducción en español , en la parte inferior.
👍👍👍👍👍👍.mantap
High freq tig
For initial arc...correct
Not continuous
Hi Chris, is the Lightning 225 available in Europe? Finland/Estonia?
I'm pretty sure these everlast machines are the same as r tech which is available in the UK
@@ronniehaycraft4052 They are not the same. They have the same case, but the internals are VERY different.
@everlast welders is the lightning 225 available in Europe, and if so, can you give me an adress?
@@a.bakker64 Not yet, but soon.
These are the ones who come to me, bring in drops, and they can’t stably hold the additive in the weld pool.
Hope it is useful
👍
"A good arc length is between 10-20 thousands of an inch"
What? This is ridiculous
10 thousands is 0.254mm