[English] How to write a WPS (Welding Procedure Specification)

Поделиться
HTML-код
  • Опубликовано: 6 фев 2025
  • After watching this video you will be able to write a welding procedure specification (WPS) on your own.

Комментарии • 136

  • @AhmedSaeed-lw5gb
    @AhmedSaeed-lw5gb Год назад

    all i can say is beautiful, no gibberish here or there stuff. direct to point and with examples and precise info.

  • @manojr2282
    @manojr2282 5 лет назад +21

    the most awaited videos sir..
    even bosses or seniors what I had seen are not willing to share their knowledge because of their ego and selfishness
    you are doing a great thing sir
    thank you so much👍👍👍

    • @WeldingandNDT
      @WeldingandNDT  5 лет назад +2

      Thank you. Please visit my website www.weldingandndt.com

    • @anewyoutuber
      @anewyoutuber 3 года назад +4

      It’s not an Ego. But they are just afraid if you are going to be better than them. Its more political than selfishness. Anyway.. happy learning..

    • @pvenkatesh7730
      @pvenkatesh7730 3 года назад

      Right

    • @jaisudhikshs7503
      @jaisudhikshs7503 2 года назад

      @@WeldingandNDT sir what is the P number for mild steel A5.1

  • @jamienoh6726
    @jamienoh6726 4 года назад +9

    I had WPS class before for a week and paid 200USD. But this 30min. lecture is much better. thanks sir. from Korea

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @evolati12
    @evolati12 4 года назад

    This right here is one of the main things that makes RUclips great: good, informative, free education. Sometimes a little difficult to understand but hey you can’t bitch when it’s free and the guy knows what he’s talking about!

    • @WeldingandNDT
      @WeldingandNDT  4 года назад +1

      Thank you. Please visit my website www.weldingandndt.com/

    • @evolati12
      @evolati12 4 года назад

      Welding and NDT Will do. Appreciate it.

  • @sohailjameel5989
    @sohailjameel5989 2 месяца назад

    Really good knowledge sharing

    • @WeldingandNDT
      @WeldingandNDT  Месяц назад

      Thank you. Please join my channel to appreciate my work, joining link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @ansari4417
    @ansari4417 3 года назад +1

    I am very happy to see this video it's very helpful for us

    • @WeldingandNDT
      @WeldingandNDT  3 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @hameedahmed748
    @hameedahmed748 4 года назад +1

    great video,i learned a lot from your comments and professional wording

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @muhamedsafvan7524
    @muhamedsafvan7524 2 года назад

    Great job well done sir👍👍

    • @WeldingandNDT
      @WeldingandNDT  2 года назад

      Thank you. Please join my channel to support my initiative. Joining Link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @titofernandezl
    @titofernandezl 4 года назад

    Good video
    No lag
    Points explained
    Easily understandable
    full star rating for this

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @Twenty_four_into_seven_vlogs
    @Twenty_four_into_seven_vlogs 9 месяцев назад

    Productive videos thank you sir

    • @WeldingandNDT
      @WeldingandNDT  9 месяцев назад

      Thank you. Please join my channel to support my initiative. Joining link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @XTREND_KSA
    @XTREND_KSA 4 года назад +2

    Sir, you are a life saver!

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @rubangrg
    @rubangrg 5 лет назад +3

    Sir You are great to share your knowledge,

    • @WeldingandNDT
      @WeldingandNDT  5 лет назад +1

      Thanks. Please visit my website weldingandndt.com

  • @SaifKhan-hg7so
    @SaifKhan-hg7so 7 месяцев назад

    Great 🎉🎉🎉

    • @WeldingandNDT
      @WeldingandNDT  5 месяцев назад

      Thank you. Please join my channel to support my initiative. Joining link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @mahasindhudey9264
    @mahasindhudey9264 2 года назад

    Very good and help full. Thank you

    • @WeldingandNDT
      @WeldingandNDT  2 года назад

      Thank you. Please use the below link to join my channel: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @amalababu91
    @amalababu91 Год назад

    Really Good content ✨🤝✨ Thanks 👍

  • @ahmadmohammed6225
    @ahmadmohammed6225 2 года назад

    Than you very much sir ..
    I have learned a lot from this vedio ..

    • @WeldingandNDT
      @WeldingandNDT  2 года назад

      Thank you. Please join my channel. Joining Link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @KrishnaDas-cq3kh
    @KrishnaDas-cq3kh Год назад

    Very excellent Sir. Thanks a lot

    • @WeldingandNDT
      @WeldingandNDT  Год назад

      Thank you. Please join my channel to support my initiative. Joining link:
      ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @anilkumarsahoo6785
    @anilkumarsahoo6785 4 года назад

    Very nicely explained.

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @thirupathieppapula5026
    @thirupathieppapula5026 4 года назад

    Great and your teaching and it help me alot thank you

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @aravindjothimurugan2201
    @aravindjothimurugan2201 3 года назад

    Nice video and good work. 👏👏👏👏
    You explanation was very nice and clear-cut. Keep going and put more videos , you will be more fame in near future.
    Looking forward to your next video 👍

    • @WeldingandNDT
      @WeldingandNDT  2 года назад

      Thank you. Please join my channel to watch all the videos. Joining Link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @chidiiwegbula7424
    @chidiiwegbula7424 4 года назад +1

    Thank you for sharing your immense knowledge..well done sir

    • @WeldingandNDT
      @WeldingandNDT  4 года назад +1

      Thank you. Please visit my website www.weldingandndt.com/

  • @allinonebyakk7878
    @allinonebyakk7878 2 года назад

    Awesome 💥🙏

    • @WeldingandNDT
      @WeldingandNDT  2 года назад

      Thank you. Please join my channel to watch all the videos. Joining Link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @mohamedferoz2913
    @mohamedferoz2913 2 года назад

    Good video content

    • @WeldingandNDT
      @WeldingandNDT  2 года назад

      Thank you. Please join my channel to support me. Joining link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @karthikeyanvenkatraman4715
    @karthikeyanvenkatraman4715 3 года назад +3

    Excellent presentation sir please show each table from the standard and please fill all tables with an example in the next video. That will be really helpful

    • @WeldingandNDT
      @WeldingandNDT  2 года назад

      Thank you. Please join my channel to support me. Joining Link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @GyanPrakash-po7bn
    @GyanPrakash-po7bn 4 года назад

    excellent presentation and with all tech details ,regards

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @ismaeljamin7987
    @ismaeljamin7987 8 месяцев назад

    Very good explanation

    • @WeldingandNDT
      @WeldingandNDT  8 месяцев назад

      Thank you. Please join my channel to support my initiative. Joining Link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @farhaniftikhar2379
    @farhaniftikhar2379 4 года назад

    You have done a great job.
    Thanks for the lesson.

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @paramasivamsubbiah3742
    @paramasivamsubbiah3742 4 года назад

    nice very clear and you made it easy sir

  • @mohamedabdou3384
    @mohamedabdou3384 3 года назад

    Great Effort From You, Thanks So Much

    • @WeldingandNDT
      @WeldingandNDT  3 года назад

      Thank you. Please join my channel to watch all the videos. Joining link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @SumkalSam
    @SumkalSam 4 месяца назад

    Should there be different wps for groove , fillet joints....?

  • @jyothisthomas2705
    @jyothisthomas2705 5 лет назад +1

    Thanks for your efforts sir

  • @simonwong6172
    @simonwong6172 3 года назад

    Very informative, thank you.

  • @mr34chanti
    @mr34chanti 4 года назад

    U should write all the points.. codes is not required keep it up sir. Please do another video with all overview of points

  • @fvsood
    @fvsood 5 лет назад +1

    Great video !

    • @WeldingandNDT
      @WeldingandNDT  5 лет назад

      Thanks. Please visit my website weldingandndt.com

  • @mppramosh8940
    @mppramosh8940 5 лет назад +1

    Great work sir thank you very much sir

    • @WeldingandNDT
      @WeldingandNDT  5 лет назад

      Thanks. Please visit my website weldingandndt.com

  • @srinivassai4696
    @srinivassai4696 4 года назад

    Thanks for your explanation and it's helpful 👍😀😁

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @noblepayyappilly7913
    @noblepayyappilly7913 Год назад

    If we preparing wps for 25 mm plate process gtaw+smaw how we get the deposit weld metal for gtaw and smaw

  • @rahulprasannan5553
    @rahulprasannan5553 3 года назад

    Super class

  • @kajjumaideen8561
    @kajjumaideen8561 Год назад

    Thank you 🎉

  • @ramu041
    @ramu041 2 года назад +1

    Sir,for weld overlay what is thickness range ( pqr and wqt)if deposited weld metal is 2mm in 1inch plate .And the what should be the total width to be deposited in pqr and wqt

  • @SumkalSam
    @SumkalSam 4 месяца назад

    Asme is very confusing.....for a single welding process...wps for plate , pipe will be different?

  • @abderrahmanebenabdallah672
    @abderrahmanebenabdallah672 5 лет назад +1

    Great work thank you sir

    • @WeldingandNDT
      @WeldingandNDT  5 лет назад

      Thanks. Please visit my website weldingandndt.com

  • @rudycesneros5122
    @rudycesneros5122 4 года назад

    Thank you very much for knowledge sharing.

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website for notes, videos and other important informations www.weldingandndt.com/

  • @raeesshaikh6678
    @raeesshaikh6678 4 года назад +1

    Great knowledge but
    In PWHT T for thickness of Material not you mentioned it (Temperature 22:59 to 23:13 please refer it )

  • @musondampandashulu6470
    @musondampandashulu6470 5 лет назад +1

    Hey Nandeep, just watched WPS writing video in English. Very educative. Thanks lots. Would you also touch PQR`s, like when you need a new PQR?

    • @WeldingandNDT
      @WeldingandNDT  5 лет назад

      Thank you. I will upload videos on PQR too. Please visit my website www.weldingandndt.com

  • @sandeepchaubey5567
    @sandeepchaubey5567 5 лет назад +4

    Sir please explain about backing
    And how to find A No for different welding consumables

  • @mohammedkadhim9483
    @mohammedkadhim9483 4 года назад

    hi sir i have Q is that applied on storage tank or only for piping?

  • @raufbasra2116
    @raufbasra2116 5 лет назад +2

    Sir please make video on material test certificate

  • @swapnilkawade3218
    @swapnilkawade3218 2 месяца назад

    Great expectations

    • @WeldingandNDT
      @WeldingandNDT  Месяц назад

      Thank you. Please join my channel to appreciate my work, joining link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @savanraval1489
    @savanraval1489 3 года назад +1

    1-2 mm should be there for root face instead of 1-2 m; overall video is so helpful
    Keep uploading more videos

  • @hamzarasheed1232
    @hamzarasheed1232 3 года назад +1

    @26:26 For specifications of shielding gas, the correct name is SFA-5.32 in ASME Section II Part C (2019)

  • @naouelsalematia9325
    @naouelsalematia9325 3 года назад

    Thank you so much

    • @WeldingandNDT
      @WeldingandNDT  3 года назад

      Thank you. If you want to financially support me, Please join my channel. Joining Link: ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @mehmetatar443
    @mehmetatar443 5 лет назад

    Good video and giving many details, I think, if you have time you should get one more time this video to clear explanation, thank you

    • @WeldingandNDT
      @WeldingandNDT  2 года назад

      Thank you. Please join my channel to support my initiative. Joining Link:ruclips.net/channel/UCH7nXSievFlbRKzKzEySbkwjoin

  • @tanveerahmed6525
    @tanveerahmed6525 5 лет назад +1

    Dear Sir ,
    Your way of presentation is Awesome And Thanks a lot for Sharing your valuable knowledge
    Can you plz make a video on Demand of Job market based on coating inspector Courses like SSPC/B-GAS/NACE CIP LEVEL-1 & 2 ..Which will be better Among those

    • @WeldingandNDT
      @WeldingandNDT  5 лет назад

      Thanks a lot. Please visit my website www.weldingandndt.com/

  • @mani4r
    @mani4r 5 лет назад +2

    Will you please start teaching important chapter of ASME code. If you are planning so please reply.

  • @tapaspanda50
    @tapaspanda50 3 года назад

    Sir make a video on Piping Execution Engineer related questions and answers for interview .

  • @liyakatsherasia8377
    @liyakatsherasia8377 5 лет назад +1

    request to make video on how to review MTC

  • @nidhishknk501
    @nidhishknk501 4 года назад

    Thank you

    • @WeldingandNDT
      @WeldingandNDT  3 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @rao416able
    @rao416able 4 года назад

    Please make a video on the use of UCS 66 CURVE for charpy test exemption criteria

  • @praveenav7330
    @praveenav7330 3 года назад +1

    Sir, please explain how do I write , specification type and grade of material in WPS.

  • @mutazmumin
    @mutazmumin 5 месяцев назад

    What about pipe diameter?

  • @abdulsamee1223
    @abdulsamee1223 4 года назад +1

    How we are selecting F & A number
    For F number we can select 7018, 6010, 7010 etc any one we can select or can we refer any table for F Number for and particular material for this filler ???

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      For F no and A no for a filler material there is table in ASME sec IX.
      Thank You. Please visit my website www.weldingandndt.com/

  • @afzalsaifi4946
    @afzalsaifi4946 3 года назад

    What is SFA specification of GTAW welding for carbon steel filler wire?
    SFA 5.9 or 5.18

  • @praveenav7330
    @praveenav7330 3 года назад +1

    Hi sir, please let me know how to write "specification type and grade " in WPS. as per Qw.422 Specification SA (asme) , but all WPS having ASTM specification. How can I know ASTM specification table ? And one more question, eg. For p number 1 material there are lot of material specification in Qw. 422 how can I select which material specification need to write in WPS table ? Sir please answer my question.

  • @begobi007
    @begobi007 5 лет назад +2

    How to fix heat input limits(max)? Is there any reference code for that? I know formula.

  • @priyankavincent1880
    @priyankavincent1880 4 года назад

    sir which ASME section we can get the interpass temperature details?? kindly reply

  • @sougatasen8537
    @sougatasen8537 3 года назад

    Electrical characteristics in not clearly understood by me Sir.. please sir tell me how to write electrical characteristics...

  • @begobi007
    @begobi007 5 лет назад +1

    Why A number mandatory and why there is no such a thing (A No) for dissimilar materials is not a mandatory?

  • @shortvideos5513
    @shortvideos5513 5 лет назад +1

    Please make video on Bgas (coating Inspector)

  • @souravbohrays4189
    @souravbohrays4189 4 года назад

    try for clad and overlay wps that will be great

    • @WeldingandNDT
      @WeldingandNDT  4 года назад

      Thank you. Please visit my website www.weldingandndt.com/

  • @jithmonnp8128
    @jithmonnp8128 5 лет назад +1

    Hi can you upload a video regarding RTFI

  • @rubangrg
    @rubangrg 5 лет назад

    Dear Sir, i have a confusion in wps, pqr and welder qualification.. My question is who is eligible to write and qualify the above. Or do we need CWI or any special welding inspector to write and qualify.. Need your valuable advice..

    • @sahebhussain8503
      @sahebhussain8503 5 лет назад

      Contractor will give pwps.based on pwps tpi/client conduct eqt&PQT and send test coupon in lab for DT test.after meeting requirement result as per code & construction ,wps will qualify/approved

    • @rubangrg
      @rubangrg 5 лет назад

      @@sahebhussain8503 thanks a lot.. 😊😊

  • @sadiksaiyed1774
    @sadiksaiyed1774 3 месяца назад

    Good evening sir refinary ki piping isometric drawing kaise read kare wo please bataiye gulf ke piping interview ka hot questions hai bahot bar puchta hai client sir.

  • @MrPravean
    @MrPravean 2 года назад

    Dear sir I am your you tube subscribe video is good useful tips I need help regarding clear explanation regarding ApI 1104 specially different type of welder qualifications can you make video about this

  • @muhammedsalih7284
    @muhammedsalih7284 5 лет назад

    For shielding gas, it is not SFA-5.3.2. It is SFA-5.32

  • @himanshukatakiya6340
    @himanshukatakiya6340 5 лет назад +1

    Unable to download it...
    Plz help

  • @ashishghadiya9578
    @ashishghadiya9578 5 лет назад +1

    Sir, I enjoy and learn welding concept in detail from your videos.Thank you very much for knowledge sharing.
    If you have any questions list(With answer if possible) regarding welding and pressure vessel fabrication which may help in interview,please share with us or drop me mail if possible.

    • @WeldingandNDT
      @WeldingandNDT  5 лет назад

      Thanks. Please visit my website weldingandndt.com

  • @ramraj7701
    @ramraj7701 5 лет назад +1

    Not both root face.one is root gap

  • @shahroohsmdw842
    @shahroohsmdw842 5 лет назад

    Please do the video on ASME sec VIII

  • @vaibhavpawar3535
    @vaibhavpawar3535 26 дней назад

    Last ka 5 Min sahi se explain nai huva

  • @SarfarazAlam-pb5rn
    @SarfarazAlam-pb5rn 5 лет назад +2

    Hindi me Sir

  • @arshad5850
    @arshad5850 2 года назад

    Is it useful for cswip 3.2 or cswip 3.1?

  • @arshad5850
    @arshad5850 2 года назад

    Sir how to know which table to refer?