  • @debabrotadas7556
    @debabrotadas7556 5 месяцев назад +1

    Thank you, sir from IITK, for this beautiful explanation.
    A small request to you, sir: please make another video regarding the physical significances of %Recovery, Jnr, Jnr_diiff, G*, sin delta, etc. and how they change with temperatures, stress levels, aging criteria, etc.

  • @rahebhafezzadeh8033
    @rahebhafezzadeh8033 2 месяца назад

    Thank you for the clear explanation. I enjoyed the content and learned many things. It would be even better (or my recommendation) to show the test procedure and Inputting the required data on DSR software to run the test. I mean how to input data on the software and run the test.

  • @constructionpediajobopenin2097
    @constructionpediajobopenin2097 9 месяцев назад +2

    Sir, Please prepare one video on performance test like 2 point bending, 4 point bending , etc

  • @karuneshsrivastava6975
    @karuneshsrivastava6975 8 месяцев назад

    sir in RTFO test what is shear modulus , phase angle & shear viscosity ?

    • @SatishIITR
      @SatishIITR  8 месяцев назад +1

      They have the same meaning in RTFO test also. Shear mdulus is applied stress divided by resulting strain. Phase angle is the lag between the applied stress and resulting strain.

  • @OmPrakash-eh3np
    @OmPrakash-eh3np 6 месяцев назад

    jnr difference pass nhi aa rha kyakarna chahiye

    • @SatishIITR
      @SatishIITR  6 месяцев назад

      It means binder is not meeting the rutting criterion. Change the source of the binder.

    • @OmPrakash-eh3np
      @OmPrakash-eh3np 6 месяцев назад

      @@SatishIITR ok sir, please let me know how to improve jnr difference in PMB 76E-10 grade.