I sent a damaged motorcycle cylinder to these guys in 2019. The inside AND outside looked brand new. I tried hard to find any blemish. It was literally perfect. I’ll never EVER consider another company. Lifetime customer here.
Could you please point out the resource for me, where TRW is mentioned as Inventor of Nikasil. All informations that i could find was that MAHLE invented the coating in 1967 for the inner coating of rotary Engines (Wikipedia and other resources). Even the pending patend is registered on MAHLE.
I sent a damaged motorcycle cylinder to these guys in 2019. The inside AND outside looked brand new. I tried hard to find any blemish. It was literally perfect. I’ll never EVER consider another company. Lifetime customer here.
my left ear enjoyed this
I was about to comment the exact same ^^
Easily solved, download an equalizer for chrome or firefox that has an option for mono sound. Just click it and its fixed
Could you please point out the resource for me, where TRW is mentioned as Inventor of Nikasil. All informations that i could find was that MAHLE invented the coating in 1967 for the inner coating of rotary Engines (Wikipedia and other resources). Even the pending patend is registered on MAHLE.
How do you put 100,000 miles on a Harley, my ass would fall off, I've had mine since 1996 and I think it's got maybe 55,000 on it.
on the top of a trailer
Piece of cake...
you push it
I have seen a lot of Harleys with 100k plus. I also was in shock the first time I saw one.
Can I get any comparable data for heat transfer or friction for NSC plating and hard chrome plating?
Can you apply this coating to a blind bore?
Yes but the bore will never see it
@@baby-sharkgto4902 🤦♂
@@beachboardfan9544sorry, I couldn't resist 🤣
ofc, all alu cil chainsaws have it
But is it applied by electric arc spraying or in some other way?
electro plating
Arc spraying is how they usually apply the coating !!
If it's so hard you need diamonds to hone it how can you then say it's really weak with dirt, are you suggesting dirt is harder than diamond?
Removing material by abrasion and accurately machining something with a tolerance of -.000”+.0005” are two completely different things.
'Moly'? I heard 'moly', but I don't know what you are referring to. Thank you.
Molybdenum Disulfide Coating
Mahle company. "MAH-luh" in German. "Molly" in English.
How much for 1980 kawasaki ke 175d NSC coating
Please visit our cylinder replating page for all pricing and service options at: www.millennium-tech.net/serviceInfo.php?id=7 thanks!
Tree fiddy.
Is it possible to do this at home?
No sir. Its a very specialized process. We are 1 of only three facilities in the US and by far the largest.
Mescalinum Sunshine 😂what the hell are you on about!
DIY NIKASIL > ruclips.net/channel/UCHRXYmO1vdp-Bi1-w11R7WQ
@@H3x4L0g I think, that's why we all are here ;)
@@MillennTechnologies wrong, 2 stroke stuffing did it in his garage.
what could possibly the cost of replating a really worn out nikasil coated 2 stroke liquid cooled cylinder?
$224.95
@@MillennTechnologies I see, thanks.
When you are ready, you can use our online service order form located here: www.millennium-tech.net/serviceOrder.php
@Kevin Stearns currently using a cast iron sleeve on my liquid cooled bike. just asking how much it would cost
@Kevin Stearns I see. I should enjoy what I can enjoy right now. Hope you can ride again.
ask bmw and jag views on it. it cost them millions in replacement engines
??????????????