  • in this video i will show you how to make gold solution for silver plated
    #howtomakegoldsolution
    #jewelryplating
    #rosegoldplatedjewelry
    #platingsolution

Комментарии • 390

  • @jadenephrite
    @jadenephrite 2 года назад +73

    Thank you for your video. Regarding 0:40, the chemical formula for Potassium Cyanide is KCN. Caution must be used whenever handling cyanide, because cyanide could be fatally poisonous if it is ingested, inhaled or absorbed through bare skin. Regarding 2:25, combining 1 part nitric acid + 3 parts hydrochloric acid produces nitrohydrochloric acid, which is also known as Aqua Regia. Regarding 7:43 gold electroplating solution, if pure gold is used on the anode instead of stainless steel, then the gold electroplating solution will last much longer. This is because the gold cations in the electroplating solution will not become depleted since they will be replenished from the gold anode.

    • @expgame71
      @expgame71 2 года назад +7

      Is potassium cyanide mandatory for the proper functioning of the plating? Is it possible to replace it with another chemical element that is easier to find?

    • @jadenephrite
      @jadenephrite 2 года назад +11

      ​@@expgame71 Thank your question. Gold electroplating can indeed be performed without the use of cyanide. Alternatives to the use of potassium cyanide is to use either sodium gold sulfite or to use potassium gold sulfite.

    • @expgame71
      @expgame71 2 года назад +3

      @@jadenephrite ok thank you for your reply. How to make sodium gold sulfite and potassium gold sulfite, is nitric acid needed?

    • @expgame71
      @expgame71 2 года назад +3

      @@jadenephrite yes but the problem with the solutions already made is that it is very expensive for very little gold, I would like to be able to make it myself

    • @aru_1396
      @aru_1396 Год назад

      What is the toxicity percentage of potassium cyanide used and what is the grade of KCN

  • @vishalsambrekar
    @vishalsambrekar 2 года назад +1

    Thank you so much.i am goldsmith .i am watching everywhere,asking everyone bu they dont tell me how to make gold plating solution.your video is best instructor to me. thanks

  • @HR_SAINI
    @HR_SAINI 2 года назад +6

    You are teaching a masterpiece💗💗

  • @cabulingue
    @cabulingue 3 года назад +2

    Terima kasih banyak Pak Anif G, Saya doakan bapak selalu sehat, banyak rejeki n berumur panjang teruslah bikin konten yang bermafaat.
    pak cara buat yg rose gold itu pakai campuran CU tadi ya,
    salam

    • @AnifG
      @AnifG  3 года назад

      Amin.. terimakasih banyak om..🙏..iya betul om untuk rosegold saya pakai Cuso4/terusi.. atau bisa juga pakai yang sudah menjadi larutan

  • @vishwanathsah8657
    @vishwanathsah8657 3 года назад +4

    No one explained like this well done bro

  • @leleaquino1312
    @leleaquino1312 Год назад +4

    Thank you for your video. In Brazil I didn't find any video talking about the chemical part of gold solutions
    How many times can this solution be used? Can I use up to how many grams of jewels without losing the gold?

  • @marinnicolae4215
    @marinnicolae4215 2 года назад +23

    A nickel coating is required beforehand because the silver or copper atoms migrate to the outside and discolor the gold

    • @2ndPortal
      @2ndPortal Год назад +4

      Why, his attempt looked great. Are saying with time?

    • @travismiller5548
      @travismiller5548 Год назад +1

      Why nickel comes before chrome as well.

    • @lenny108
      @lenny108 9 месяцев назад +1

      Some say the best is to have chrome. On Amazon they sell gold electrolyte that is supposedly abrasion resistant. How is this achieved? Abrasion-resistant gold plating?

    • @RahulPatel-kk1ci
      @RahulPatel-kk1ci 9 месяцев назад +2

      nickel or chrome coating is good but not good for the skin so avoid to do

    • @newmonengineering
      @newmonengineering 8 месяцев назад +4

      ​@RahulPatel-kk1ci if you don't use nickel, the silver will tarnish under it and slowly discolor the gold. Most gold plated things are a very thin coating of gold. You can however go thicker to say 2.5 microns and it's a much better protection but also significantly more costly to do. Often they will use rhodium as a base layer over silver if they don't use nickel

  • @alejandrogracia4448
    @alejandrogracia4448 3 года назад +11

    This is priceless, thank you so much! 🙏

    • @AnifG
      @AnifG  3 года назад +1

      Thank you so much sir😊🙏

  • @vanjasemic8198
    @vanjasemic8198 3 года назад +3

    I cant believe!!!! Its wonderful!!! Congratulations

    • @AnifG
      @AnifG  3 года назад +1

      Thank you so much 😊🙏

  • @sirbinyamin7636
    @sirbinyamin7636 2 года назад +3

    Hello, Can you let us know where did you get all the chemicals you are using? because in my country I try over and over but it is simply impossible to find them or they want to sell them by huge quantity... thanks 😀

  • @nilupul84
    @nilupul84 2 года назад +2

    Hi Dear, I try it gold plating is really good. but something wrong in my solution. some brown dust making on SS Anode.
    can you tell me. HCL,HNO3,KCN & Water quantity for 250mg 24k Gold .
    Thanks

  • @avivhanale3174
    @avivhanale3174 3 года назад +4

    Hello sir can you tell me how to make brighter for this solution

  • @MrMo7emad
    @MrMo7emad 3 года назад +2

    İ don't know how to thank you
    İt's very useful video

    • @AnifG
      @AnifG  3 года назад

      You're welcome, sir 😊🙏

  • @dongbotang
    @dongbotang 3 года назад +1

    Great video! Many thanks from Australia.

    • @AnifG
      @AnifG  2 года назад

      Thank you so much.. greetings 🇮🇩

  • @phool289
    @phool289 3 года назад +2

    Very easy to understand thank you so much 💝

  • @Gazanferylmaz
    @Gazanferylmaz 3 года назад +2

    Will, we encountered a problem such as gold sinking over time?

  • @hermanrany3325
    @hermanrany3325 2 года назад +1

    Assalamualaikum bang, mau nanya.
    Bagusan mana sepuh merah dulu atau sepuh putih perak dulu sebelum proses sepuh emas?🙏

  • @algeriano5424
    @algeriano5424 2 года назад +1

    please, if we want the color of green gold and blue for example, what sulphate is needed to achieve it, and a thousand thanks for this important video, I await your answer

  • @machruskenzo7346
    @machruskenzo7346 2 года назад

    Thanks you very much 👍,,, good luck bro 👍

  • @karangandhi5216
    @karangandhi5216 3 года назад +5

    Hello sir,
    Thank you for ur vedio
    If we dissolve 1 gm how much gms we can polish for 24k

  • @detectormaniaindonesia8131
    @detectormaniaindonesia8131 2 года назад +2

    Any working PH for this plating? Thanks

  • @manishkumarpatidar7000
    @manishkumarpatidar7000 3 года назад +3

    VERY USEFUL THANKS.A LOT.

  • @randimadanthanarayana3839
    @randimadanthanarayana3839 2 года назад +1

    Thank u sir. Its really helpful for me. Sir, i did this same as your video. And i plated. Rings, pendents. after plating its really nice and success. But it is not possible for chains. Chains are got black and very ugly colour. Can plz advice me sir.

  • @MetalGearIV
    @MetalGearIV 2 года назад

    wow you are a gift for humankind

  • @solmaz.khorashadi
    @solmaz.khorashadi Год назад

    Thank you for your helpful video. I have a QUESTION, is it possible to make the rosegold solution into rosegold powder?

  • @rajasasitepu9531
    @rajasasitepu9531 7 месяцев назад

    Bang Anif, sdh like n subscribe. Saya sdh tonton video part 1 dan 2 ini. Makasih. Tapi nanya ini, apakah semua obat/zat kimia itu bisa dibeli bebas di toko kimia? Itu aliran listrik saat ngerendam cincin, pake brp volt itu bang. Thanks.

  • @jaspergold4589
    @jaspergold4589 3 года назад +3

    Please can you use 18karat gold to make the gold plating solution?

    • @AnifG
      @AnifG  3 года назад

      Thanks for watching... I can't seem to do it

  • @ricojuliusretardo7510
    @ricojuliusretardo7510 Год назад

    Thank you for sharing your Idea ,I really appreciate in you😁

  • @amyelaja3614
    @amyelaja3614 3 года назад +1

    Bang numpang nnya juga ni sama ahlinya..
    Kalao untuk pemerah harus pakai potassium cyanide..
    ?? Yang berapa persen bang..??
    Makasi infonya..

  • @takishidz7961
    @takishidz7961 2 месяца назад

    Does it need a precise voltage amont to use and does it have any impacte on the final result

  • @dusanstanic1462
    @dusanstanic1462 3 года назад +4

    Can stainless steel be plated and what is the procedure (preparation etc)? And how durable is this plating? Thank you

  • @deskmat9874
    @deskmat9874 6 месяцев назад

    Good to know I'm not the only one who writes electroplating with a k sometimes just because I felt like it

  • @pbjsilverstudio4882
    @pbjsilverstudio4882 3 года назад +2

    Saved this video!! Thanks!

    • @AnifG
      @AnifG  3 года назад +1

      Yes ma'am.. thank you very much 😊🙏

  • @johnkaka1000
    @johnkaka1000 Год назад

    Thank you so much. It’s a great help.

  • @sirbinyamin7636
    @sirbinyamin7636 2 года назад +5

    Hello, does anyone know where to buy those products? A internet site or any other place would be really helpful. Thank you very much

  • @GILBERTOMARTINEZSAUCEDO
    @GILBERTOMARTINEZSAUCEDO 10 месяцев назад +2

    Hi! my stainless steel plate started to corrode during the plating process, and contaminated the solution (green/orange) sediment do you know why this is ?

  • @harishrajamani4922
    @harishrajamani4922 3 года назад +3

    How to make cyanide free gold polishing Solution?

  • @mohideenanver3700
    @mohideenanver3700 2 года назад

    Thank you so much for sharing plating process

  • @ishqesahil8864
    @ishqesahil8864 2 года назад +1

    Anif I want to gold plate surgical instruments. Can you please tell me what proportions of ingredients are used in yellow gold plating and what is the lifetime of this plating?

  • @gonzalovaldez8204
    @gonzalovaldez8204 3 года назад +7

    Hello, it is an interesting process, when you brown a ring, the liquid that remains is discarded no longer works, how resistant is the gold, how do I make it last longer, I have seen you do other processes of black. as it does. can you teach me. saludos desde Colombia

    • @akhmadfazar7004
      @akhmadfazar7004 2 года назад

      Kalo buat 100 potong emas brp takaran emas untuk di larutkan?dan talaran hno3 sama hcl nya jadi brp gan?🙏

    • @muchniksolo4980
      @muchniksolo4980 2 года назад

      @@akhmadfazar7004 biasanya dijitung dr berat mas yg akan di plaiting,aku sendiri jg buat dgn cara itu utk bahan emas 0,25grm dpt menghasilkan kurang lebih 1kg,semoga membantu🙏

  • @sofiahearts4625
    @sofiahearts4625 3 года назад +1

    Best video thanks..........👍

    • @AnifG
      @AnifG  3 года назад

      Thank you so much 😊🙏

  • @sgj85
    @sgj85 2 месяца назад

    And what about if we want to do this this process inverse from liquid to solid gold?

  • @georgejosh1873
    @georgejosh1873 3 года назад

    Bang itu air merahnya kalo ga dicampur sama yang emas bisa buat dasaran sepuh ga? Biar merah dulu baru disepuh emas gitu?

  • @chrissmith841
    @chrissmith841 Год назад

    Does it work out much cheaper making it yourself than buying ready made? thank you

  • @dannysoni3518
    @dannysoni3518 3 месяца назад

    Does we need surface activator for gold plating on silver ... if yes tjen how can i make that

  • @wawanrustiawan1201
    @wawanrustiawan1201 3 года назад +1

    Pak hanif. Kalau mau ngelapis emas di cincin berbahan stainless, ga bisa langsung kaya di video ya? Apa ada tambahan campuran khusus?

    • @AnifG
      @AnifG  3 года назад

      Kalo untuk stainless gak bisa bang..ini cuma bisa untuk melapisi tembaga, alpaka, perak sama emas

  • @randyreyes8689
    @randyreyes8689 Год назад

    Thank you for your video, thank you very much

  • @sonuverma2796
    @sonuverma2796 4 месяца назад

    How much volt and amp did u use for gold and rose gold plating

  • @franknieto2760
    @franknieto2760 3 года назад +3

    Potassium cyanide is very deadly. Where can you get it? Other than gloves and good ventilation, what precautions should one take?

    • @AnifG
      @AnifG  3 года назад +1

      yes it is very poisonous, I think a lot of materials for the jewelry production process are toxic, the important thing is to always maintain work safety with the right procedures

    • @armazrivera2302
      @armazrivera2302 3 года назад

      There is an internet page where you can find potassium cyanide

  • @takishidz7961
    @takishidz7961 2 месяца назад

    Is there any special specification of the chemicals you using for this experiment

  • @BALITEKNIK070809
    @BALITEKNIK070809 3 года назад +1

    Wow mantap tutorialnya, sukses buat channelnya

    • @AnifG
      @AnifG  3 года назад

      Terimakasih om.. sukses juga buat anda 😊🙏

  • @user-mp6vf3xg7v
    @user-mp6vf3xg7v Год назад

    Hello,
    I have prepare the plating solution as per your instructions, but the colour of the plating is black in colour. Please clarify. We want to know the exact amount of HCL and HNO3. Thank you.

  • @user-yk9ee4jk1u
    @user-yk9ee4jk1u Год назад

    Thank so mach for this interesting video but i am just wondering of using potassium or potassium cyanide

  • @takishidz7961
    @takishidz7961 2 месяца назад

    I want to know what is the density of the hno3 and HCl

  • @Bhuvikasoni
    @Bhuvikasoni 3 года назад +1

    Love from india

    • @AnifG
      @AnifG  3 года назад

      Thank you so much 😊🙏

  • @Fashion.jpeg_
    @Fashion.jpeg_ 2 года назад

    Can this solution be used on 3d printed items? Do I need to spray anything on the 3d printed item first if so?

  • @nyomanngetis6329
    @nyomanngetis6329 Год назад

    Maaf boss, untuk sepuh rose gold apakah bisa buat ketebalan tertentu?

  • @sliceofbrain_
    @sliceofbrain_ 2 года назад

    Thankx for sharing your knowledge. May I know what is name of the electric machine you are using. And where can I buy it?

  • @aitamerabdrrahim7823
    @aitamerabdrrahim7823 Год назад

    Please how do I get the 18k paint solution what is the composition

  • @sudhar889
    @sudhar889 4 месяца назад

    Hello sir is hcl and nitric acid concentrate on diluted? Please tell 😢

  • @flight3624
    @flight3624 3 года назад +3

    How to maintian the bath for large scale production of rose gold

    • @AnifG
      @AnifG  3 года назад +3

      It is only suitable for small scale, for large scale production I have never tried🙏

    • @faisalishfaq5877
      @faisalishfaq5877 3 года назад

      @@AnifG contect naber

  • @hobiaja7666
    @hobiaja7666 3 года назад +1

    Ada yg jual air sepuhan jadi tinggal pake nggk mas yg kayak itu.....?
    Terimakasih

    • @AnifG
      @AnifG  3 года назад

      Di toped ada bang

  • @isawalter3465
    @isawalter3465 3 года назад +4

    Hello Anif, could you PLEASE show us, how to get the gold out again of the solution, like somones asked already? That would be so great!

  • @gamelife7139
    @gamelife7139 11 месяцев назад

    Hi Bro, thank you for video
    have a Quistion
    How make lemon yellow color for gold plating? (mean lighter yellow than 24k like lemon)
    thank you❤

  • @kushalmaulloo762
    @kushalmaulloo762 2 года назад +1

    Hi, i used the same process for 24k plating, but 1/2 quantity.
    But my jewelleries turned black and dull..
    What did i do wrong please?

    • @wahyukuncorojati66
      @wahyukuncorojati66 Год назад

      Terlalu lama ketika proses pewarnaan di dalam airnya. Menjadikan barang kusam. Cara untuk memulihkannya kembali dengan cara di poleshing. Dan di proses kembali.

  • @rayaraya6720
    @rayaraya6720 Год назад

    Potasium pakai potas apa ya mas agar air sepuhan tidak cepat berubah keruh

  • @armazrivera2302
    @armazrivera2302 3 года назад +2

    Can it be applied on pieces of steel ???

    • @AnifG
      @AnifG  3 года назад +2

      No, it can only be used for gold, silver and copper

    • @armazrivera2302
      @armazrivera2302 3 года назад +1

      @@AnifG If I cover the steel with copper, will it work?

  • @mochamadvidal4186
    @mochamadvidal4186 Год назад

    Mantap boss.
    Kalau boleh tahu, tinggalnya dimana..?

  • @tonykarlsson8589
    @tonykarlsson8589 Год назад

    Good job 😊

  • @helloitsanxiety6234
    @helloitsanxiety6234 Год назад

    hi! what about silver 925 plated things? i have a necklace that is indian silver, since it's old and i cleaned it very aggressively last time, a brassy color came out 🥲so now i have a necklace that is a spotted coloration 😭i was thinking of coating it in silver 925 but i don't know how...i'd like to do it myself cause i'm poor but my dad used to make handmade jewelry so i have some equipment, also i like to learn new things. could you hand me some tips? thank you so so much
    (also i'm form italy so forgive my poor english pls)

  • @armazrivera2302
    @armazrivera2302 3 года назад +3

    Hello Angie, how much water do you need? 0.5 grams or 1 gram

    • @AnifG
      @AnifG  3 года назад +3

      For 1 grams of gold you need about 6 ml of HCL and 2 ml of HNO3

    • @armazrivera2302
      @armazrivera2302 3 года назад +2

      @@AnifG thanks how many grams of cyanide potassium do I need and how many milliters of water to dissolve it I am about to do it I got 0.5 gram 24k gold

  • @sudendiyali1983
    @sudendiyali1983 Год назад +1

    What type of water is this

  • @satheeshkumar-un6rl
    @satheeshkumar-un6rl 2 года назад

    Superb demonstration

  • @plumbum1153
    @plumbum1153 9 месяцев назад

    Excellent !!!!

  • @bernardkorley6946
    @bernardkorley6946 Год назад

    So how long will such a playing last normally before you would have to plate it again

  • @famtovar5385
    @famtovar5385 9 месяцев назад

    So can you reuse the gold solution after one time? If so how many times can i reuse it…. And should i remix with the rest of the solution (unused solution) ?

  • @dariovelasco7336
    @dariovelasco7336 3 года назад +2

    Como preparas tu solución para.blanquear tus piezas

  • @jacquesomersavard7257
    @jacquesomersavard7257 2 года назад

    is it possible to make this whit stain glass copper frame or lead frame

  • @anandpanchal6390
    @anandpanchal6390 3 года назад +1

    Thanks for share your precious experience
    How much ml Hno3 and Hcl for 2 gram gold

    • @AnifG
      @AnifG  3 года назад +1

      for 2 grams of gold, you need about 10 ml of HCL and 3 ml of HNO3

    • @anandpanchal6390
      @anandpanchal6390 3 года назад

      @@AnifG million of thanks sir🙏🙏

  • @alexandrerodrigues3531
    @alexandrerodrigues3531 Год назад

    Parabéns!
    Belo trabalho 🙏

  • @erickvidianto1215
    @erickvidianto1215 3 года назад +1

    Hallo om..semoga sukses selalu..saya ada pertanyaan om..berapa lama waktu untuk mencairkan logam emasnya om? Dan yg warna biru itu apa namanya..semoga dijawab..terimakasih om..udah saya like dan sub.

    • @AnifG
      @AnifG  3 года назад +1

      Hallo bang terimakasih sudah mampir..untuk mencairkan emasnya gak lama bang sekitar 1-5 menit, jangan terlalu panas kompornya bang.. dan untuk yang warna biru itu namanya tembaga sulfat bang (CuSo4) atau (terusi).. di toped ada harganya sekitar 60-80 rb an per kg.. dipakai sedikit aja 0,5 gram per liter kalo kebanyakan bisa hitam hasilnya

  • @pratishshrestha9623
    @pratishshrestha9623 3 года назад +1

    How long does it last??

  • @sachinlohar1106
    @sachinlohar1106 3 года назад +1

    Sir isme kitna kam niklta hai

  • @jacquesomersavard7257
    @jacquesomersavard7257 2 года назад

    I have lot of electronic gold part is it possible to use it in this process

  • @arifinpanegoro6882
    @arifinpanegoro6882 2 года назад

    Pakai berapa volt mas? Apakah voltase juga pengaruh ke kekuatannya?

  • @ccezar84
    @ccezar84 3 года назад +2

    Hello Anif. How thick can you plate with this solution without getting dull? Can you achive 2 microns of bright gold plating?
    This solution plate on non-ferous only? How good is the adhesion?

    • @AnifG
      @AnifG  3 года назад +1

      Thanks for watching, I don't understand the answer to your question, but as far as I am it is the cheapest way to get the gold solution, and I always use it

    • @isawalter3465
      @isawalter3465 3 года назад

      can you please explain that ? I just know this channel and never saw, he says something about dumbness beyond 2 microns ... sorry german but the guy is super experienced ..
      ruclips.net/user/RolandBetzmannRealGoldvideos

    • @isawalter3465
      @isawalter3465 3 года назад +1

      @@AnifG Hi dear Anif, amazing! I am following this channel. He recommends 3micron for average use up to way more depening on purpose.
      Is your solution limited regarding micron thickness? thank you! Are you on Facebook for PN? thank you! :-)

  • @alexsinlae5876
    @alexsinlae5876 3 года назад +2

    Untuk gold colornya gmn ?? Makasih

    • @AnifG
      @AnifG  3 года назад

      Untuk pewarna emas bisa pakai auruna bang.. tapi gak usah dicampur potas..cukup larutan emasnya aja..

  • @kutubsk2105
    @kutubsk2105 3 года назад +2

    Very nice and

    • @AnifG
      @AnifG  3 года назад

      Thank you so much

  • @EnriqueGuerreroO
    @EnriqueGuerreroO 3 года назад +2

    If I want to 18K gold electroplate a carbon knife (opinel), can I use as anode a piece of 18k jewelry, and, as I don't have a gold solution, can I use simple sodium bicarbonate as my electrolite?

    • @AnifG
      @AnifG  3 года назад

      I don't understand about that, maybe someday I'll try to experiment about it

    • @AbdulKareem-lq3tr
      @AbdulKareem-lq3tr 2 года назад

      Assalamu alaikum Haneef jee how to make cheepest gold solutions would yu pls reply

  • @hengkifernando4063
    @hengkifernando4063 3 года назад +1

    Mksh banyak ilmunya bg,itu kalau pakai air sepuh yg hambar buat campuran rose goldny boleh gk bg,trus klo hambarnya air rose gold itu di celupin warna jd apa bg

    • @hengkifernando4063
      @hengkifernando4063 3 года назад

      Mohon petunjuknya bg

    • @AnifG
      @AnifG  3 года назад +1

      Air sepuh hambar itu gimana bang? Itu saya pakai air aquabides bang dicampur potas sama CuSo4..nanti pas mau pakai dikasi air emas dikit perbandingan (1:3)

    • @hengkifernando4063
      @hengkifernando4063 3 года назад

      @@AnifG mksh banyak bg🙏,mksudnya air emas bekas yg udh di celupin pengganti air emasny bisa bg?

    • @AnifG
      @AnifG  3 года назад

      Oh iya bisa bang.. sy juga kadang pakai air emas bekas bang

    • @hengkifernando4063
      @hengkifernando4063 3 года назад

      @@AnifG maaf bg agak banyak tanya🙏🙏,tp hasilnya bagusan mana bg ya,dan bedanya apa bg

  • @techsvayrieng3280
    @techsvayrieng3280 Год назад

    Good brother,thank you.
    Have Other solution for make it bright or not?

  • @MegaUsman42
    @MegaUsman42 3 года назад +2

    Can you please tell, how much time per mg is required. Or how much time is sufficient to electroplate jewellery

  • @hargrim6892
    @hargrim6892 3 года назад +1

    @Anif G, HCl sama HNO3 itu pakai yang berapa persen ya? kalau di pasaran saya lihat ada yg 32% sama 65%

    • @AnifG
      @AnifG  3 года назад

      Semakin tinggi kadar kemurnian ,semakin bagus bang,,

  • @nurettingencturk1124
    @nurettingencturk1124 Год назад

    are we going to neutralize three parts of hydrochloric acid and one part of nitric acid ? thanks.

  • @byanarga2387
    @byanarga2387 3 года назад +1

    Thank you so much

  • @thetruth1989
    @thetruth1989 Год назад

    Sir how do you get the 24k gold color not yellow gold color

  • @InfinityJewellery06
    @InfinityJewellery06 2 года назад

    Can 14k gold be played in this solution

  • @kndblade
    @kndblade 3 года назад +1

    Definitivamente eternamente agradecido, muchísimas gracias saludos

  • @billmusik9794
    @billmusik9794 8 месяцев назад

    Is that just plane potassuim?

  • @hyperhidrosissupport9186
    @hyperhidrosissupport9186 11 месяцев назад

    can i use potassium ferrocyanide instead of cyanide ?