Thanks . I studied for a while , I must admit I watched a lot on Dusan999 and Omgageek, I have refined just over 2 kilos of silver and just 23 grams of pure gold
I like this channel cuz it’s close to what I am doing. Right now I’m doing eco-goldex leeches followed by electrolysis. I going to try wound copper wire as the cathode so I can drop it right into the copper cell. Have’t done yields yet.
Are you using the Eco leech to selectively remove gold from circuit boards and pins ? I have to incinerate the filtrate and papers from removing the silver in the slimes now .
@ Yeah. I was going to incinerate what was left over. ChatGPT suggested leeching over incineration. I’m not even going to crush them. My current batch is crushed broken solar cells. I put them in a rock polisher with large ball bearings. I have heard you can used grain shredders for pc cards and memory but I’m going to try this first.
Sorry anode although in the eco goldex they seem to reverse after a day or so and you get a precipitate which they say has good stuff also. I then drop the ph (outside as it offgasses cyanide) and precipitate with zinc wire. I’m still playing around with it obviously.
@ I’ll keep posting. I have my own atomic absorption spec I just haven’t set it up as I need venting. The benefits of Eco goldex is that I should be able to pop samples right into the AA. With nitric you have to raise the ph which is a pain in the ass.
Sweet ! That's a nice bit of silver from the slimes ! I really appreciate the mention and thank you on doing the GAW ! First time I've won anything!
You got it !
Love watching lower budget refining always makes me think I could do it
You can I studied for a couple of years then decided to do it
Thanks . I studied for a while , I must admit I watched a lot on Dusan999 and Omgageek,
I have refined just over 2 kilos of silver and just 23 grams of pure gold
That's a real nice fume hood you made, I like setup.
Work in progress . Need to complete the copper cell run , so I can do upgrades on it
I like this channel cuz it’s close to what I am doing. Right now I’m doing eco-goldex leeches followed by electrolysis. I going to try wound copper wire as the cathode so I can drop it right into the copper cell. Have’t done yields yet.
Are you using the Eco leech to selectively remove gold from circuit boards and pins ?
I have to incinerate the filtrate and papers from removing the silver in the slimes now .
@ Yeah. I was going to incinerate what was left over. ChatGPT suggested leeching over incineration. I’m not even going to crush them. My current batch is crushed broken solar cells. I put them in a rock polisher with large ball bearings. I have heard you can used grain shredders for pc cards and memory but I’m going to try this first.
@naughtiusmaximus830 I think that you might be on to something
Sorry anode although in the eco goldex they seem to reverse after a day or so and you get a precipitate which they say has good stuff also. I then drop the ph (outside as it offgasses cyanide) and precipitate with zinc wire. I’m still playing around with it obviously.
@ I’ll keep posting. I have my own atomic absorption spec I just haven’t set it up as I need venting. The benefits of Eco goldex is that I should be able to pop samples right into the AA. With nitric you have to raise the ph which is a pain in the ass.
Nice kitty!
I’m dying , she’s a bad ass
😂 she wants to know who your talking to lol
She’s something alright she loves the garage and the dog never more than a few feet apart now