Hi I'm using epifanes yacht enamel thinned at 10% but I'm still getting orange peel, but I desire a glass finish, it's 14°C, here in the UK... Would adding a little easy flow help to reduce flash time, I'm finding it flashes in seconds almost instantly, thinned at 5% it left a lot of holidays curtains and orange peel. I'm only using epifanes products and working very quickly. I also used a test board and found 10% to be the optimum result. Anymore and the blue colour starts becoming translucent and wants to curtain on me. I found if I apply too thinly the flash time is even faster. I'd like improve and be able to apply glass like coatings to both my own and other people's boats... (with dreams of becoming an epifanes sponsored pro) Any tips for getting that last coat to flow out like glass when using alkyd yacht enamel?
Hi I'm using epifanes yacht enamel thinned at 10% but I'm still getting orange peel, but I desire a glass finish, it's 14°C, here in the UK...
Would adding a little easy flow help to reduce flash time, I'm finding it flashes in seconds almost instantly, thinned at 5% it left a lot of holidays curtains and orange peel.
I'm only using epifanes products and working very quickly. I also used a test board and found 10% to be the optimum result. Anymore and the blue colour starts becoming translucent and wants to curtain on me.
I found if I apply too thinly the flash time is even faster.
I'd like improve and be able to apply glass like coatings to both my own and other people's boats... (with dreams of becoming an epifanes sponsored pro)
Any tips for getting that last coat to flow out like glass when using alkyd yacht enamel?
Do you have a product you sell that you recommend for a Aluminum bass boat? I plan on just painting over the paint that is already there.