    @leonelrey729 3 года назад +2

    Garret, thank you sir for your help today over the phone!

  • @jacobbraden301
    @jacobbraden301 2 года назад

    Dry material. If it is hygroscopic. Up injection speed, or psi. ,but not enough to sheer. And a drowling nozzle could be a bad heater band or thermocouple . And make sure you barrels are at the right temp.. if you have valve gates that can affect your plastic flow aswell

    • @michaelburks7928
      @michaelburks7928 Год назад

      What bout if a valve gate tip is excessively bigger than the other one, like close to resembling a stop sign lol?