Hi, for amorphous polymers you should be seeing multiple glass transition regions during the heating/cooling cycle. You can look up the data sheets to see which polymer has glass transition at that temperature or you can do an FTIR analysis to check for the peaks and find out the polymers. You can watch the FTIR video in our channel to learn more
@@mediwise2474 with DSC, you will be able to find out the glass transition temperature. Combine this with FTIR, you can find the family of polymer ex. PC-ABS will have two dips in the DSC indicating 2 glass transitions, and in FTIR curve you can see peaks that are characteristic to these 2 materials.
🔥🔥🔥
how to confirm amorphous copolymer by dsc
Hi, for amorphous polymers you should be seeing multiple glass transition regions during the heating/cooling cycle. You can look up the data sheets to see which polymer has glass transition at that temperature or you can do an FTIR analysis to check for the peaks and find out the polymers.
You can watch the FTIR video in our channel to learn more
@@microlabtesting sir how to correlate dsc of amorphous copolymer with ftir
How ftir supports dsc of amorphous cooolyner
@@mediwise2474 with DSC, you will be able to find out the glass transition temperature. Combine this with FTIR, you can find the family of polymer ex. PC-ABS will have two dips in the DSC indicating 2 glass transitions, and in FTIR curve you can see peaks that are characteristic to these 2 materials.