Numerical on allowance|shrinkage allowance

Поделиться
HTML-код
  • Опубликовано: 5 ноя 2024

Комментарии • 11

  • @prsrpattanaik
    @prsrpattanaik Год назад

    Hi... Sir...
    This is a hollow component and there will be 10 mm wall thickness per side.
    As the shrinkage depends on the Material and thickness so will it shrink same as a solid part.

  • @jalajbhatt5451
    @jalajbhatt5451 3 года назад +1

    Thank You So much for the detailed explanations

    • @KDEDUTECHE
      @KDEDUTECHE  3 года назад

      thank you for giving feed back

    • @piyushmane9995
      @piyushmane9995 3 года назад

      @@KDEDUTECHE why negative allowance for that cavity sir.. can you explain briefly.. please..🙏

    • @sampathchary9155
      @sampathchary9155 3 года назад

      @@piyushmane9995 because in regular metals the inner diameter (cavity) increase in size after casting

  • @yusufal.mehaizia7737
    @yusufal.mehaizia7737 Год назад +1

    80-1.6=78.4

  • @nileshadole9714
    @nileshadole9714 Год назад

    Sir wht is standard draft allownce angle for different materials i.e steel aluminium

    • @KDEDUTECHE
      @KDEDUTECHE  Год назад +2

      For metal pattren taper is 50 % of hard wood pattern (given below)
      Height of. Wall. External. Internal
      51-100. 1.2 mm. 2.5 mm
      101-200. 1.8 mm. 3.5 mm

    • @nileshadole9714
      @nileshadole9714 Год назад

      @@KDEDUTECHE Thank you sir for your support

  • @abhayawasthi9345
    @abhayawasthi9345 3 года назад

    Thank you!