Under Size welds:Visual Welding Acceptance Criteria : AWS D1.1 welding defects: Part 3
HTML-код
- Опубликовано: 3 окт 2024
- video about welding inspection education
It covers topics below
welding defects covered in AWS D1.1
acceptance criteria for the welding defects
weld size
under size weld
this video is helpful for the person who is preparing for the welding inspection certifications like CWI , CSWIP , ICC or BS . Good for engineers who want to learn about welding symbols in detail.
Type in comment below for any suggestion or information.
very well explined about undersizes with examples sir.. thank you soo much.
I appreciate your comment
sound quality is defected....its very difficult to understand. Length of under size weld is , L=.5"
Then, what is U=? Clear this one.Please....
Hello Tapon, I know that. during early days of my youtube I was struggling for the editing. I am improving daily , thank you for the feedback
Thank You!
Very Useful!
PDF format of it would have been very handy.
Please share if you could.
Armen Miskarov MSCE
3rd degree connection3rd
Armen has a account
OneWeb Senior Civil Structural Engineer
can not add you Sir :(
Nice explanation and I would like to say thanks and it is also requested to you please make a video on weld defects for static tubular and cyclic tubular so that topic could be cover fully about defects
I have one doubt.. I didn't understand size and under size. Pls explain me detaily
size is asked in the drawing by design engineer, underside means actual measurement which is different from the drawing
Sir great very helpfull
i really appreciate your comment , do you want to learn anything specific ?
Please do a video on welding consumables
Sure, any specific suggestion about this topic ?
I mean what you really want to know ?
this field is huge and it will help me to ensure your need
@@weldinginspection7239 from the point of view of cswip 3.1 exam
@@nabeelgaffar sure , i will do that especially for you :)
Sir what is the terminology in PJP joint can Ultra sonic test applicable as compare to CJP joint
yes, but it depends on technician's skill and sometimes it gives false positive. best way to do it is to make sample coupon similar to actual joint, calibrate the machine and check the weld
QUESTION 1
LENGTH IS