  • @cazadoresdenortecarolina1410
    @cazadoresdenortecarolina1410 8 месяцев назад +2

    🔥🔥🔥🇬🇹🇬🇹

  • @carloswelding4257
    @carloswelding4257  8 месяцев назад +1

    Hello guys, thanks for commenting, it sounds like that because the temperature is high, the voltage is 27 and the wire is 555, that's why it sounds like that, we solder like that and thanks for watching the video 😉

  • @bobomounten3098
    @bobomounten3098 8 месяцев назад +1

    Greetings from Macedonia 🇲🇰 excellent weld👍

    • @carloswelding4257
      @carloswelding4257  8 месяцев назад +1

      Thank you friend for watching my video and greetings from Macedonia 🇲🇰

  • @glocca254
    @glocca254 8 месяцев назад +3

    Looks like the shield gaas is being blown or not high enough flow , judging by the weld comtamination

    • @skyraider87
      @skyraider87 8 месяцев назад +1

      That's just silica mate

  • @ciroromeo903
    @ciroromeo903 7 месяцев назад +1

    Troppo filo