  • In this video Zac Buchanan talks about his approach to cleaning up the solder joint on his Loveless style knives.
    He talks about buffer safety, the tools he uses in polishing his knives and shows you the way he buffs the tight corner where the guard meets the blade.
    Zac talks about the tool and the technique he uses to shave off the excess solder around the joint to get a nice clean finish on the sides of the blades ricasso.
    Zac then shows the results of his work on “How to make a presentation grade solder joint"!
    Remember to hit the Like and Subscribe buttons if you’d like to see more content like this! Thanks for watching!!

Комментарии • 37

  • @ChristopherSalisburySalz
    @ChristopherSalisburySalz 2 года назад +2

    That buffer/grinder is the real deal!! That thing runs really well and it looks like it has a ton of power.

  • @rhysmcv7875
    @rhysmcv7875 3 года назад +1

    Yup, another very good one, with tons of helpful advice about the process that I've not managed to find anywhere else. Thanks so much

    • @ZacBuchananKnives
      @ZacBuchananKnives  3 года назад

      You’re welcome. I’m glad it’s helpful.

    • @rhysmcv7875
      @rhysmcv7875 3 года назад

      @@ZacBuchananKnives super helpful from a theoretical standpoint. Practically speaking I still need to put in the time and effort, but still... if you'll take a shooting (or archery) analogy: at least now I have a target to shoot and and know how to hit it, it's just the practice now. Thanks again

  • @hawintherknives4386
    @hawintherknives4386 10 месяцев назад

    Love your work man

  • @silvergoldking
    @silvergoldking 3 года назад +1

    That was cool. Thanks for sharing.

    • @ZacBuchananKnives
      @ZacBuchananKnives  3 года назад

      Of course, I’m happy to share. Thanks for the comment

  • @heikolang335
    @heikolang335 Год назад

    Got yourself a new subscriber 👍

  • @richardpreisler3352
    @richardpreisler3352 Год назад

    Damn, that is beautiful !

  • @VFSFRI
    @VFSFRI 4 года назад

    Amazing work.

  • @Jasoncohenour
    @Jasoncohenour 3 года назад

    TY Zac, good safety tips, and how-to, now I know about brass rod trick ! What kind of mask / filter are you using?

  • @GARYMANDIEVAN
    @GARYMANDIEVAN 2 года назад

    Hello Zac where do I find that yellow compound I have been using green

  • @dgundeadforge17
    @dgundeadforge17 2 года назад

    what solder do you use. Sorry found video. I love your work. I was able to watch a documentary on loveless and you should be very proud of your work.

    • @ZacBuchananKnives
      @ZacBuchananKnives  2 года назад

      m.ruclips.net/video/qQLJiliDQSc/видео.html here is a link to part one. Let me know if it works.

  • @kostadinpecanov5797
    @kostadinpecanov5797 Год назад

    Hi Great knife May I ask how to make such a tool to clean the cotton disc Thanks

  • @charlieratliff1488
    @charlieratliff1488 3 года назад +1

    Good video. Lots of helpful tips here. Could you link where you got that rouge from? Thanks. Great looking
    Knife.

    • @ZacBuchananKnives
      @ZacBuchananKnives  3 года назад

      Thanks! Let’s me know if this doesn’t work.
      www.riogrande.com/product/rio-sunsheen-bobbing-compound-pre-polishing-compound/3315001

  • @griffithshandmade-knives
    @griffithshandmade-knives 3 года назад +1

    Zac have you had the opportunity to meet either Steve Johnson or Jim Merritt?

    • @ZacBuchananKnives
      @ZacBuchananKnives  3 года назад +1

      Yes, I’ve met Steve several times, he is a very nice guy and a great maker. I met Jim a couple times at the CCKS, he was a very nice and genuine man, RIP.

    • @griffithshandmade-knives
      @griffithshandmade-knives 3 года назад

      @@ZacBuchananKnives that is very cool. I’d never have had the opportunity up here in Canada obviously, but great to hear you did👊👍

  • @kostadinpecanov5797
    @kostadinpecanov5797 Год назад

    Здравейте Страхотен нож
    Може ли да попитам как да си направя такъв инструмент с който да почиствам памучния диск Благодаря

  • @TwistedGorillaFab
    @TwistedGorillaFab 2 года назад

    She's a beaut!

  • @sanyok7777
    @sanyok7777 3 года назад

    Zac good afternoon Would you be so kind to tell me what kind of paste flux or kit you are using it to soldering I would greatly appreciate

    • @ZacBuchananKnives
      @ZacBuchananKnives  3 года назад

      It’s a long weird name, check out “how to make a presentation grade solder (pt1)” 5 minutes 32 seconds in. 👍

    • @sanyok7777
      @sanyok7777 3 года назад

      I see
      Would you be so kind to tell me what type of wire do you use for soldering is it silver Stay shine or what is the name of it

  • @jeanmartiny527
    @jeanmartiny527 9 месяцев назад

    why not TIG soldering ? is your soldering strong enough ?

    • @ZacBuchananKnives
      @ZacBuchananKnives  9 месяцев назад

      The guard is pinned and soldered. So yes, it will be plenty strong enough for it’s purpose and use.

  • @howardmcclain9784
    @howardmcclain9784 9 месяцев назад

    I thought you said blade down for safety.

  • @santosknives6278
    @santosknives6278 4 года назад

    Buffing looks SCARY!

    • @ZacBuchananKnives
      @ZacBuchananKnives  4 года назад +1

      Fernando Soltero Yeah, you want to stay focused. But as long as you use proper technique and caution it’s pretty safe.

  • @johnrizzato9192
    @johnrizzato9192 Год назад

    I’m not sure why you buffed it before you used the brass rod

    • @ZacBuchananKnives
      @ZacBuchananKnives  Год назад +1

      Buffing helps remove excess and gives you a better visual on what you need to remove. There’s a lot of back and forth with these knives, polishing just to mess it up and polish again

  • @bryanbaker6767
    @bryanbaker6767 3 года назад +1

    Great video.....wire wheels are nasty and dangerous can’t tell you how many times they have ripped parts out of my hand

    • @ZacBuchananKnives
      @ZacBuchananKnives  3 года назад +1

      Very true, I only use it for applying “orange peel” texture to Titanium. Thanks for the comment

  • @quentinnothling4991
    @quentinnothling4991 3 года назад +1

    Should be called how to clean a joint not how to make a solder5 joint