  • @Lovelyblog237
    @Lovelyblog237 4 года назад

    Sir hamre yaha gi ki sheet h powder coated ki usme pin hole bahut aa raha h kya karu bolo

  • @myfoundryworld569
    @myfoundryworld569 3 года назад

    What do you mean by"gas dissolved in metal charge"??
    Can you please explain how it occurs...

  • @narendrageete1467
    @narendrageete1467 2 года назад

    Sir,In cover casting wall thickness 2.5mm we are facing out gassing issue after powder coating [ Glossy Black] ,Please give suggestion how to overcome

  • @yadavyogesh5082
    @yadavyogesh5082 3 года назад

    Micro porosity ka problem he sir to kya kare

  • @CGLwarrior14
    @CGLwarrior14 4 года назад +1

    👍👍

  • @mathguru8084
    @mathguru8084 5 лет назад

    nice

  • @niteshkumarcnc8139
    @niteshkumarcnc8139 5 лет назад

    Bore gauge ka vedio daliye Sir ok

  • @yadavyogesh5082
    @yadavyogesh5082 3 года назад

    Ok thanks

  • @niteshkumarcnc8139
    @niteshkumarcnc8139 5 лет назад

    Dail snap gauge setting karne ka vedio daliye Sir ok