  • This video is about Sample Calibration Procedure for a Zero Degree PAUT Application such as Corrosion Inspection.

Комментарии • 17

  • @NDTVideoLibrary
    @NDTVideoLibrary  5 лет назад +3

    Download the Phased Array App from google play store. Just search "PAUT Buddy" or follow this link: play.google.com/store/apps/details?id=com.saurabh_lawande.NDT

  • @calvinburkhalter1563
    @calvinburkhalter1563 8 лет назад +1

    Thank you so much...Your explanation was clear and concise.

  • @nrmr6527
    @nrmr6527 8 лет назад +2

    1velocity...2wedge delay and 3sencibility....
    the omniscan use the velocity of the material to calculated the delay of the wedge....that is the reasons

    • @pratikwagh6467
      @pratikwagh6467 8 лет назад

      That's correct! The wedge is made of Perspex and the instrument thinks it is Mild Steel.

    • @nrmr6527
      @nrmr6527 8 лет назад +1

      +Pratik Wagh....olympus madr the wedges whith Rexolite....w/acustic propieties closer to water

  • @kmandinga8070
    @kmandinga8070 8 лет назад +1

    This video changed my life

    • @NDTVideoLibrary
      @NDTVideoLibrary  8 лет назад

      Good to hear that.

    • @kmandinga8070
      @kmandinga8070 8 лет назад

      Ok, maybe it didn't change my life....but Pratik is a great teacher, and his passion for others to learn is evident.

  • @nithikasn
    @nithikasn 6 лет назад +1

    Hi Wagh
    Calibration Procedure for a Zero Degree PAUT Application such as Corrosion Inspection is useful
    I have a PAUT task on 95mm carbon steel block cladded with 3mm SS 316L
    How to fabricate this block and wherto put holes
    either SDH required or FBH required
    need your suggestion

    • @NDTVideoLibrary
      @NDTVideoLibrary  6 лет назад

      Hi Na v, you have to have a clad block of same thickness and cladding. All you need to calibrate for is wedge delay. Reference Sensitivity: First BW from 95 mm should be set to 80% FSH. No TCG needed so you do not need FBH or SDH unless you are also looking for volumetric defects and not just corrosion. And then map any reduction in thickness. Report like C Scan with different color indicating remaining thickness.
      Note: this is just a suggestion. Refer to your company procedure before performing inspection.

  • @nerijusvaickus1449
    @nerijusvaickus1449 3 года назад

    Hi, how you remove signal from wedge if you testing let's say 100mm thick plate?

  • @debbiebueno3371
    @debbiebueno3371 4 года назад

    Hi sir. I have questions sir. Omniscan sx is capable for HDPE pipe (high density polyethylene)?