1. Platinum Crucible ka jaga Nickel Crucible use kiya jaa sakta hai ? 2. hamara Yeha fusion mixture k jaga 4-5 pice sodium hydroxide plates crucible mai de ke fuse korta hai. Fuse karne ka Yeh wala process thik hai na ? 3. Bumb na kare ishi liye Percloric acid k jaga kuch or use kar sakte hai ? 4. Bikar mai Pehela 1:1 Hcl beg hone ke badh thanda karke hamara yeha 10ml dm water and 10ml sulfuric acid bikar mai dhalke fir hitter mai rakh ke beg karne ke badh 1:1hcl deke dissolve karne k badh filter karta hai. Yeha wala process sahi hai ? 5. Fuse karne time aur last mai jalane ke time Muffel furnace ka temperature kitna hota hai ? 6. Silica ka jo Calculation nikla hai uske sath silicone ka factor into (×) karke jo nikle ga wohi silicone Aajaye ga na ? .4816÷5 × silicone factor (46.72)
Thank you sir
❤❤❤
Sir, could you make a video on ferro alloy phosphorus analysis please??
Sir Please Fe2O3 ka bhi video bna dijiye…
Sir nfc ka cr2o3 test ka video de sakte hai kya?
Sir aap bole solution ka fe2o3 hoga, plz ek baar test ka video daliye, or pehle aap daal chuke hai to boliye
Sir nickel analysis ki bhi video banaiye
Ramming mass me boran ka testing kaise karte hai sir iske bare me ek video banaye sir
Sir, namaskar
Sir aap kis plant se ho
Mujhe coal ka moisture nikalne ka formula btao to
Sir please sodium silicate ka analysis ka bhi video dale please
sir alumina ka IS method me bna dijiye
Boric acid % test in ramming mass video upload kare sir
How to analyse boron in ramming mass
First view
Sir, Good mng
Can I make a contact analytical method
To find out caco3 content in calcite powder
❤
❤ we have Ppt sio2 powder want to test fe2o3 in this.pls upload ur analysis video ❤
Thanks
Boric acid ka or dal do sir
Please make a video on casteble
Sir please makes a video related to find the gas content (CO2) of the incoming river sand
Sir , ak video carbon testing pe v banaiye ..step by step
Kiska carbon
@@analysismethodbykumarsatya3694 mild steel ka
@@analysismethodbykumarsatya3694 sir mild steel ka
Sir mild steel ka, aap jab video bana dete hai to hum sab k pass ak guid k roop me save rahta hai bahot help hota hai ...
Silica crucible fuse kr sate hai kya sir y sirf platinum crucible only
No silica crucible me nahi hoga
Sir please make a video on ferro Chromium request sir
Ok
Sir Fe (m) me or fe (t) me kya aandar hai
Fe(m) metalic iron
Fe(t) Total iron
sir perchloric acid bole na
Yes
hello sir ,
Mera kuch question thaa , agar ho saketo jabab dijiye ga..
1. Platinum Crucible ka jaga Nickel Crucible use kiya jaa sakta hai ?
2. hamara Yeha fusion mixture k jaga 4-5 pice sodium hydroxide plates crucible mai de ke fuse korta hai.
Fuse karne ka Yeh wala process thik hai na ?
3. Bumb na kare ishi liye Percloric acid k jaga kuch or use kar sakte hai ?
4. Bikar mai Pehela 1:1 Hcl beg hone ke badh thanda karke hamara yeha 10ml dm water and 10ml sulfuric acid bikar mai dhalke fir hitter mai rakh ke beg karne ke badh 1:1hcl deke dissolve karne k badh filter karta hai.
Yeha wala process sahi hai ?
5. Fuse karne time aur last mai jalane ke time Muffel furnace ka temperature kitna hota hai ?
6. Silica ka jo Calculation nikla hai uske sath silicone ka factor into (×) karke jo nikle ga wohi silicone Aajaye ga na ?
.4816÷5 × silicone factor (46.72)