Another good one OWL!! 10/10 for metallurgy and chemistry. 10/10 for production and content. I am even getting to like your music. Keep up the great work!!
Super nice👍how can i get rid off paladium from gold solution dont have dmg or formic acid ? Need help the solution has gold and paladium an a bit off silver
Why are ceramics able to go into the crucible right away and the plastic ICs had to be incinerated first? I have no experience with processing material like this besides for watching your videos. Just thinking about I'm guessing the plastic would melt into one piece fucking everything up, but that's only a guess. Have a good week and be safe
Great video! I assume these transistors where all T03's? And that you cut them open with an angle grinder. And only use the die and the bondwire of it, is dat correct? And do you perhaps know the total weight of the 1500 transistors?
I don't use the smelting technique to make the dore often but I am curious do you lose any gold to the slag with the sodium hydroxide at high temp? also how do you dispose of the slag? i'd assume it is like cupels and absorbed some lead? or does the mass amount of carbon absorption keep all metals from oxidizing?
Gold could be lost trough mechanical enclosure in the slag when the slag is not viscous enough, sodium hydroxide helps with slag thinning. I don't dispose of the slag, it can be remelted over and over again, or it could be converted to metal, with reducers.
Здравствуйте! ЛАЙК вам ✌️🤗. Скажите пожалуйста шо за порошок СМБ? И где он переминается! И скажите он пры осаждения золота тянит другие металлы? Спасибо большое 😉😁
Na2S2O5 - sodium metabisulfite - SMB - пиросульфит натрия при осаждения золото тянит МПГ, поетому если они присутствуют в растворе должен применяться другие редукторы - нитрит натрия, щавелевая кислота...
de-NOxing is the process of removing the free nitric acid from the solution, some people are using urea, some evaporate three times with HCl, some are using formic acid, I prefer sulphamic acid as it concerts the free nitric acid acid to sulphuric, which precipitates lead as lead sulphate if any is present. If you have an active oxidant in your solution and you don't deNOx the gold you precipitate will go back in solution
Сова фантастический результат! Лайк за великолепную работу! Интересно за счет чего такой выход? Транзисторы обычно 30мг это с количества 45г,22г с микрух это 5 мг в одной,всегда считал что в таких 2мг.
Heya ! What a great result again ! It's still too cold here to start recovery season and i feel impatient to begin. People can't imagine the time we spend on finding and preparing the ore... A question : Is it a home made crucible your are using in that vid ? Prices of all needed component to work are getting higher and higher as inflation grows... Do you feel the same dream as precious metal's prices will explode this year ? Whish you the Best. GodBless you.
I tried this method today i added 3kg lead and 50 gram silver for 3kg gold contain material finally i got 500 grms melted lead I have tested in computer machine it shows 21k gold present in this lead metal Now how to remove lead from this melted metal before dissolve in nitric Can you explain pls
@@Detalius Пока не пробовал, но уверен, что будет работать как с оптронами, так и с процессорами, завтра жду приезда партии 10 кг мостов и сниму процесс.
The best of your work is in the way you improvise tools, equipment and some containers.
Here I also make with what I have on hand.
A hug.
Another good one OWL!! 10/10 for metallurgy and chemistry. 10/10 for production and content. I am even getting to like your music. Keep up the great work!!
Hello Mr Owl.
I enjoy this clip 🙂
Thank you from Norway 🌹
Glad you enjoyed it!
Super nice👍how can i get rid off paladium from gold solution dont have dmg or formic acid ? Need help the solution has gold and paladium an a bit off silver
You can use sodium nitrite or oxalic acid
Exelent!
Thanks!
After IC incineration you did not wash just added the lead?
Yes
Can You explain how you made the forg burner is it gas or charcoal burner
Pls show the forg burner on video it will help full for me pls👌👌💐
ruclips.net/video/OsLkSK6tMls/видео.html
Why are ceramics able to go into the crucible right away and the plastic ICs had to be incinerated first? I have no experience with processing material like this besides for watching your videos. Just thinking about I'm guessing the plastic would melt into one piece fucking everything up, but that's only a guess. Have a good week and be safe
that's a good guess :) I wont be able to see if all plastic is gone which will lead to much longer holding times
Great video! I assume these transistors where all T03's? And that you cut them open with an angle grinder. And only use the die and the bondwire of it, is dat correct? And do you perhaps know the total weight of the 1500 transistors?
That's correct I was given only the dies of the TO-3s to process, so I don't know the overall weight.
Brilliant! Cheers for the effort guys! Can’t wait for the next one
Thanks for watching mate, many more to come!
You're name sounds Welsh
هل يمكن صهر القطع ألتي تحتوى البلاديوم في الفرن مباشرة وشكرا جزيلا لك ونرجوا منك التركيز على الطرق البدائية بدون الأحماض
يعتمد على المطرقة ، إذا كان يمكن الوصول إلى درجة الحرارة هذه
ما هي المطرقة وشكرا جزيلا
Just imagine how much precious metals are put into the ground every year because people just throw shit away at dumps, such a shame
Thats why I recycle 😁
I don't use the smelting technique to make the dore often but I am curious do you lose any gold to the slag with the sodium hydroxide at high temp? also how do you dispose of the slag? i'd assume it is like cupels and absorbed some lead? or does the mass amount of carbon absorption keep all metals from oxidizing?
Gold could be lost trough mechanical enclosure in the slag when the slag is not viscous enough, sodium hydroxide helps with slag thinning. I don't dispose of the slag, it can be remelted over and over again, or it could be converted to metal, with reducers.
Hi, i dont understand how the lead has extracted from the melted dore? Please can you explain.
it was oxidised to litharge and removed with the slag, google cupellation
@@OwlTech333 thank you very much
Always good to see a video from you, hope you're doing well
The was realy cool to watch. I Enjoyed it and gave it a 👍 Is that really worth it to reclaim the gold, as in the cost of time and chemicals needed?
Absolutely
Bonjour
comme toujours un plaisir de suivre les vidéos
vas me falloir le visionné plusieurs fois pour tout comprendre 👌
Здравствуйте! ЛАЙК вам ✌️🤗. Скажите пожалуйста шо за порошок СМБ? И где он переминается! И скажите он пры осаждения золота тянит другие металлы? Спасибо большое 😉😁
смб если не ошибаюсь это пиросульфит натрия. хотя незнаю зачем пишу если автор не отвечает.
Так точно!
@@OwlTech333 люблю ребусы😂😂🙈
Na2S2O5 - sodium metabisulfite - SMB - пиросульфит натрия при осаждения золото тянит МПГ, поетому если они присутствуют в растворе должен применяться другие редукторы - нитрит натрия, щавелевая кислота...
@@OwlTech333 спасибо большое 👍 я незнл шо пиросульфид так обозначают ☝️☺️
Fantastic result and video! 🌟 🌟 🌟 🌟 🌟 👍
Thank you! Cheers!
all type of ic optocoupler have a gold inside? sorry my bad english
Don’t know about all but these ones do
How is it possible to sleep in soluble water after SMB?
i think i already asked you but what are the titles of the two music tracks again?
m.soundcloud.com/owl-tech/tracks
Great job, well done sir
Thanks!
What music is playing in this video, between 00:50 - 09:13 minutes?
soundcloud.com/owl-tech/something-big?
@@OwlTech333 thank you
hello sir, is it possible to get Palladium this way?
yes ruclips.net/video/C6_hU8klfxE/видео.html
الستيل كان فيه اسمنت او لا
رقم
Nice job, love seeing the shinny :-) 👍👍
Hello sir what is de-NOxed and sulphemic acid why in use please sir answer me you very legend man
de-NOxing is the process of removing the free nitric acid from the solution, some people are using urea, some evaporate three times with HCl, some are using formic acid, I prefer sulphamic acid as it concerts the free nitric acid acid to sulphuric, which precipitates lead as lead sulphate if any is present. If you have an active oxidant in your solution and you don't deNOx the gold you precipitate will go back in solution
@@OwlTech333 thinks I am big fan
Отличная работа, простенько и со вкусом 👍👍👍😁 и выход приятный 💪 наконец то понял почему азотная кислота концетрированная а не разбавленная...
Работает быстрее, и потом получаю кристаллы нитрат серебра покажу на следующий ролик
@@OwlTech333 серебро закупоросится,и всё будет супер
Nice work sir
Thanks
✌️PT
Thank you too
Hi
Can you process 10kg gold plated pins?
How to contact you and get it done?
very nice i like gold button good job idol..
Thank you!
Результат порадовал👍👍👍
Мне тоже :)
Combien cela a coûté de produit
Excellent video as always thank you !!!! Congratulations 👏 🎊
Thanks for watching!
Nice button. Hope you wore a respirator, You just put a load of lead oxide into the air
We did wear respirators
Извените увидел серебро если не сложно какая в данном случае пропорция свинца и серебра на этот объем
Ag:Pb 1:5-10
Сова фантастический результат! Лайк за великолепную работу! Интересно за счет чего такой выход? Транзисторы обычно 30мг это с количества 45г,22г с микрух это 5 мг в одной,всегда считал что в таких 2мг.
Спасибо! Микрухи 0,007г Транзисторы 0,018-0,025
Parabéns pelo trabalho e talento owltech.
muito obrigado
Heya !
What a great result again !
It's still too cold here to start recovery season and i feel impatient to begin.
People can't imagine the time we spend on finding and preparing the ore...
A question :
Is it a home made crucible your are using in that vid ?
Prices of all needed component to work are getting higher and higher as inflation grows...
Do you feel the same dream as precious metal's prices will explode this year ?
Whish you the Best.
GodBless you.
Hi there mate, always happy to read your comments! Regarding the crucible - yes it's DIY :) crucible bottom of a natural gas cylinder (mild steel)
What is the thickness(Gage) of steel sheet 1mm (or) 2 mm
@@rightvideos5057 2.5mm the stainless steel sheet the one used for crucible is about 5mm
Great result!
Thanks!
Impresionante el sistema de purificacion 👍
Thank you!
Exelente proceso,y muy bien explicado👍
What color is copper
brown
Great work as always!⭐⭐⭐⭐⭐
Thanks again!
I tried this method today i added 3kg lead and 50 gram silver for 3kg gold contain material finally i got 500 grms melted lead I have tested in computer machine it shows 21k gold present in this lead metal
Now how to remove lead from this melted metal before dissolve in nitric Can you explain pls
You should to oxidize lead. Do it with cupellation and oxygene
ruclips.net/video/XJe5U0lOfiE/видео.html
How to extract residual gold from SMB water
Do a stannous chloride test, you wil see that there is no gold left after precipitation.
wieder mal ein sehr schönes video
Vielen Dank für Ihre Zeit!
Amazing now that's a button 👏 excellent video thank you 😊
Glad you liked it!
the disks from transistor made from molibden
Хай возник вопрос диски не метал вроде молибден почему он не сгорел
Не растворяется свинцом
Great video. Thank you. Please take care and stay safe. Talk to you later my friend. 🙂🙂🙂😇😇😇👍👍👍
Sir gold complete refined not what smb
سلام عليكم الدقيقه ٧ كان القرص فظه او ذهب او رصاص او ذهب
Ag+Au
هل يمكن وضعها في بوتقة اسمنتيه
Yea
شكرا جزيلا لك
Hihi. Yes it wat bad🌹Nice gold sir
Thanks for watching
Транзюки дали результат в основном! Но думаю что потери есть как грама 2 точно 😊
Very good 👏🏾👏🏾👏🏾👍🏾🇧🇷
Thank you!
Най добрият.
Благодаря!
Можете ли да говорите на Български език?
@@1lt3r с Google translate мога да говоря на всички езици 😊
Thanks for posting! The background music is so annoying, though, that I had to watch it with sound turned off.
Yeah I know its time to change it
I just love the music.
Video 👍 music 👎 sick of hearing it now very old, however a good job boys 👌
доброго здравия. сейчас посмотрим что Сова приготовил.))
благодарю за видео😊😊
Спасибо за просмотр!
@@OwlTech333 вы же знаете это не трудно, трудней донести полезную информацию.) удачи.
Привет, процесс интересный, навеное трудозатратный но стоит своего!
Привет! Наоборот процесс самый быстрый из тем которые я знаю, все закончилось за около 5 часов
@@OwlTech333 Я такой способ не пробовал, но итнересно а мосты от пк тоже без потерь обжигать можно твоим способом.
@@Detalius Пока не пробовал, но уверен, что будет работать как с оптронами, так и с процессорами, завтра жду приезда партии 10 кг мостов и сниму процесс.
very good
Yeah that what I'm talking about,
I am follow your video from 10 years ago and still can't produce gold button,,😂
This doesn't speak well of my videos 😂
Красавчики. 👍
Stannous Chloride after smb the color becomes brown
copper
Jast feri goood master
Holy fuck! Nice !
~$4400ish
Think pink Floyd music wd sound better Great video though
И как изготовить такую печь хочу научиться вашему искусству
Какое искусство, это самы древней аффинажный процесс
ruclips.net/video/OsLkSK6tMls/видео.htmlsi=9MYXmOsH-Xzw-ojj ruclips.net/video/1UfeWc8t4Ys/видео.htmlsi=s09w-76o-TOm1vcj ruclips.net/video/C6wIIKtsXTs/видео.htmlsi=n-fhMzUdXJZYNFQ4
@@OwlTech333 спасибо большое за ваши ответы
Muy bien.
Fantastico
Not bad 🌹
공유 감사합니다
👍👍👍👍
good
Tebrikler.
Что означает порошок смб и в ролике я не увидел серебра
Пиросульфит натрия
👍
Extraction
I think.. Hm... 98-110 gram🙂
👍👀
هذا نحاس أصفر... وليس ذهباً
هذا هو التعليق الأكثر سخافة على الإطلاق! من الواضح أنه ليس لديك حتى فهم أساسي للعمليات المعنية.
@@OwlTech333 من الواضح أنك افهم واحد في العائلة عندكم في الأساسيات المعنية...
Almost like cooking wack 😆 or recooking
عملية معقدة بدونها
🤗👍👍
فيديو راىع
شكرا سلام و صحة
ما شاء الله
Привет. Ни хрена не пойму, материал советы. Ты кто?
Привет! Я свой!
Привет удачи и здоровья
O
👍👍👍
👍