How to tell the SOAK TIME of a Hydrographic film

Поделиться
HTML-код
  • Опубликовано: 10 дек 2024

Комментарии •

  • @terrylockwood2430
    @terrylockwood2430 Год назад +1

    Another great video. You just showed me why I struggle so much with several of those films like the one on the right

  • @Dad_at_50
    @Dad_at_50 6 месяцев назад

    Just stared yesterday you guys sure make it look easy . Thank you for the videos

  • @hobbyprison
    @hobbyprison Год назад

    Thanks for the vid. Helpful! Would have liked to see how it dipped with a longer soak time.

  • @리페어맨
    @리페어맨 Год назад

    Dear Brian, Thank you so much for letting me know your know-how.

  • @Blimpus
    @Blimpus Год назад

    This was extremely helpful, Thank you for this one

  • @andrewlloyd4702
    @andrewlloyd4702 Год назад +1

    Thanks for the videos.

  • @STVenom225
    @STVenom225 Год назад +1

    Would be good if you made a film sit time on a chart for before you activate and after.

  • @brandonemmanuel4994
    @brandonemmanuel4994 Год назад

    What a legend

  • @henrysara7716
    @henrysara7716 Год назад

    Great video, thy.

  • @delonv9518
    @delonv9518 Год назад

    How do u take spray chrome off plastic parts??
    Do u have any suggestions?

  • @mohamadtivolii
    @mohamadtivolii Год назад

    thanks for the video but i would have loved to see how it dipped with the right amount of time

  • @KarterMorey24
    @KarterMorey24 Год назад

    How much film would I need to dip a shotgun I am looking to dip one but I don’t know how much film to buy

    • @LiquidConceptsUSA
      @LiquidConceptsUSA  Год назад

      We sell film in meters. 1Meter is 39.37 inches. We offer 1Meter wide film & 50cm wide film. Hope that helps.

  • @PaulCapello
    @PaulCapello Год назад

    i havent seen any "soak time" reccomendations for films on your website.

    • @LiquidConceptsUSA
      @LiquidConceptsUSA  Год назад

      All films we recommend a 60 second soak time. There are a very few that require additional soak time and those are all noted in those films product description.

  • @andrewlloyd4702
    @andrewlloyd4702 Год назад

    Can you please do a video, showing preparation, base coat choice etc, is there any list for base coats that go with the films?

    • @LiquidConceptsUSA
      @LiquidConceptsUSA  Год назад

      Most all base coats are listed on our website for each film. We do have a few separate prepping videos as well as how base colors can affect your film on our channel if you want to give it a look.

  • @jesussantibanez6711
    @jesussantibanez6711 Год назад

    👍🏼👍🏼👍🏼👍🏼

  • @MichaelSlackta
    @MichaelSlackta Год назад

    Your in house film with the plastic backing does not even begin to break down after 60 seconds as per your included instructions.

    • @LiquidConceptsUSA
      @LiquidConceptsUSA  Год назад

      Hi Michael can you shoot me an email or give me a call to discuss. This does not sound correct but I need to know more information to diagnose. Also did you watch the video with the instructions to be sure you were laying the right side on the water and using it properly?

  • @craigalex8860
    @craigalex8860 Год назад

    I’m new to hydro dipping and wanted clarification on soaking in warm or cold water what do you recommend?

    • @LiquidConceptsUSA
      @LiquidConceptsUSA  Год назад

      We recommend 80-90 degrees for your tank water temperature