Painting Adhesion Testing Using Pull-Off Method
#mistermhw #painting #coating #pressurevessel #adhesive #pqt #pulloff #trending #viral #adhesion #astm #iso #akzonobel #industrial #4k #4kvideo
@mistermhw
This video contains adhesion testing with the pull-off method. In the paint and coating industries, paint adhesion testing is often used to determine if the paint or coating will adhere properly to the substrates to which they are applied. Several tests measure the resistance of paints and coatings from substrates: cross-cut test, scrape adhesion, pull-off test, and others.
ASTM D4541
Background Music License :
@KVmusicprod
Gate by KV @KVmusicprod
Creative Commons - Attribution 4.0 International - CC BY 4.0
www.creativecommons.org/licen...
Просмотров: 664

Видео

Inserting A Tube Bundle Into An Air Cooler Heat Exchanger.
Просмотров 1,8 тыс.Год назад
Inserting A Tube Bundle Into An Air Cooler Heat Exchanger.
API 650 Storage Tank Design Engineering: Full Water Testing
Просмотров 811Год назад
API 650 Storage Tank Design Engineering: Full Water Testing
How To Do A Hydrostatic Test On A Flare Ko Drum
Просмотров 655Год назад
How To Do A Hydrostatic Test On A Flare Ko Drum
The Purpose Of Positive Material Identification In Weld Areas
Просмотров 924Год назад
The Purpose Of Positive Material Identification In Weld Areas
Hydrostatic Testing: Pressure Vessel Inspection
Просмотров 5 тыс.Год назад
Hydrostatic Testing: Pressure Vessel Inspection
Inspection Of Materials According To ASME
Просмотров 6332 года назад
Inspection Of Materials According To ASME
PREFLASH COLUMN - CRUDE DISTILATION UNIT || RDMP PROJECT WITH GRID ZOOM EFECT
Просмотров 7072 года назад
PREFLASH COLUMN - CRUDE DISTILATION UNIT || RDMP PROJECT WITH GRID ZOOM EFECT
POST WELD HEAT TREATMENT ||| PRESSURE VESSEL - CARBON STEEL ||| HEAT TREATMENT
Просмотров 2,4 тыс.2 года назад
POST WELD HEAT TREATMENT ||| PRESSURE VESSEL - CARBON STEEL ||| HEAT TREATMENT
FORMING HEAD || ELIPSOIDAL || PRESSURE VESSEL
Просмотров 25 тыс.2 года назад
FORMING HEAD || ELIPSOIDAL || PRESSURE VESSEL
Hydrostatic Test Of Tube Bundle Heat Exchanger
Просмотров 25 тыс.2 года назад
Hydrostatic Test Of Tube Bundle Heat Exchanger
SHIPPING GIANT VESSEL DOCUMENTARY - PART II || PRESSURE VESSEL || COLUMN
Просмотров 6062 года назад
SHIPPING GIANT VESSEL DOCUMENTARY - PART II || PRESSURE VESSEL || COLUMN
SHIPPING GIANT VESSEL DOCUMENTARY - PART I || PRESSURE VESSEL || COLUMN
Просмотров 3882 года назад
SHIPPING GIANT VESSEL DOCUMENTARY - PART I || PRESSURE VESSEL || COLUMN
A Simple Guide To Understanding The Tube Bundle Component Of Heat Exchangers
Просмотров 2,9 тыс.2 года назад
A Simple Guide To Understanding The Tube Bundle Component Of Heat Exchangers
Find Out How To Quickly Identify Stainless Steel With Positive Material Identification!
Просмотров 6832 года назад
Find Out How To Quickly Identify Stainless Steel With Positive Material Identification!
How To Inspection A Pressure Vessel For Hydrostatic Testing
Просмотров 17 тыс.3 года назад
How To Inspection A Pressure Vessel For Hydrostatic Testing

Комментарии

  • @Srk7028
    @Srk7028 Месяц назад

    tested with what medium ?

  • @tgplc
    @tgplc 3 месяца назад

    Estimasi harga untuk SS gr. 304 dim 1000 mm tebal 3 mm berapa ya per head

  • @shinopchacko3759
    @shinopchacko3759 3 месяца назад

    Which country..

  • @mohdfirdausosman6238
    @mohdfirdausosman6238 6 месяцев назад

    hello mister, apakah formula yg digunakan utk HT di atas?

    • @mistermhw
      @mistermhw 6 месяцев назад

      Formula yg digunakan mengacu ASME VIII Sect.I para UG-99

  • @koyahassan6137
    @koyahassan6137 9 месяцев назад

    Which pump is used to pressurise the equipment, selection of pump

  • @paksipm
    @paksipm 10 месяцев назад

    What is inspection test pressure ?

    • @paksipm
      @paksipm 10 месяцев назад

      How calculate it ?

  • @syamramadhan7447
    @syamramadhan7447 11 месяцев назад

    Mesin press 1000 ton , maximum tebel plat berapa mm

  • @supadmi3892
    @supadmi3892 11 месяцев назад

    Tebal shellnya brapa pak?

    • @mistermhw
      @mistermhw 11 месяцев назад

      Perkiraan under 20 mm. Point pekerjaan di fabrikasi bundle and insert to shell, existing shell scope client.

  • @ABHEJIMBOZ
    @ABHEJIMBOZ 11 месяцев назад

    Interesting, keep the great work and improving, never give up.

    • @mistermhw
      @mistermhw 11 месяцев назад

      Thank you bosqueee. Sukses selalu

  • @jaysukhsabaliya2415
    @jaysukhsabaliya2415 Год назад

    Which company sir ??

    • @mistermhw
      @mistermhw Год назад

      In Indonesia, with more than 50 years experience

  • @TheCazara
    @TheCazara Год назад

    Один работает трое дармоедов

  • @pedrocraft990
    @pedrocraft990 Год назад

    Amazing

  • @heryjupry4034
    @heryjupry4034 Год назад

    Info loker nya pak 🙏

  • @tiowahyudi5769
    @tiowahyudi5769 Год назад

    Proyek apa ini bng...

    • @mistermhw
      @mistermhw Год назад

      RDMP Balikpapan, Bang

    • @supadmi3892
      @supadmi3892 Год назад

      thickness brapa bang,headnya?

    • @mistermhw
      @mistermhw Год назад

      Itu head cladding bang, SA 517 Gr.70+316L, thickness 32+3 mm

    • @supadmi3892
      @supadmi3892 Год назад

      ​@@mistermhw kalo thickness shellnya brapa bang?

    • @supadmi3892
      @supadmi3892 Год назад

      ​@@mistermhw kalo thickness shellnya brapa bang?

  • @MrAndhiguy
    @MrAndhiguy Год назад

    Mantap bro

  • @Ezeleonm
    @Ezeleonm Год назад

    good video, thanks

    • @mistermhw
      @mistermhw Год назад

      U'r welcome. if you don't mind, please share my channel with your friends

  • @johntyson1998
    @johntyson1998 Год назад

    Did y'all gas fire stress relief or ues seramic heat pads.

    • @mistermhw
      @mistermhw Год назад

      depending on the dimensions, you can use a chamber, which means using gas, or a heating element/pad. The vessel in this video uses a chamber, here's the link as example ruclips.net/video/WjESqGujVVo/видео.html

    • @johntyson1998
      @johntyson1998 Год назад

      Yes I see that y'all use 20hp blower's and 10 inch.burnners. I'm a retired heat treated I really miss my work.

  • @jijovg729
    @jijovg729 Год назад

    Thanks bro

  • @kannantv1064
    @kannantv1064 Год назад

    Need to do measurement vessel expansion? With tape

    • @mistermhw
      @mistermhw Год назад

      It depends on your client or ITP request. generally what is done before the hydro test is the final inspection, the final inspection including checking the final dimensions of the vessel, pneumatic test on pads, etc. Measurement of vessel dimensions before the hydro test is mandatory

    • @kannantv1064
      @kannantv1064 Год назад

      @@mistermhw thanks 🙏

    • @mistermhw
      @mistermhw Год назад

      @@kannantv1064 Hopefully this answer can help you. If there is still something that needs to be discussed, I welcome it

  • @Sinarlas3
    @Sinarlas3 Год назад

    Pak kita mau bodem Demeter 50 cm. Tinggi 25 cm bisa kan jadi nya kaya batok gitu

    • @mistermhw
      @mistermhw Год назад

      Ada drawingnya pak? Mungkin bisa share drawingnya.

  • @naufalmoralis9701
    @naufalmoralis9701 2 года назад

    Mantap gan

    • @mistermhw
      @mistermhw 2 года назад

      Makasih bang. Bantu share vidio ke temen yg lain ya bang.

  • @xod7861
    @xod7861 2 года назад

    Used these in elreno ok. At Permian tank and vessel many different sizes to

    • @mistermhw
      @mistermhw 2 года назад

      If you dont mind. Please share my vidio to another friend.

  • @humenbot24
    @humenbot24 2 года назад

    what does that Red line Indicate?

    • @mistermhw
      @mistermhw 2 года назад

      Red line indicates temperatur.

    • @humenbot24
      @humenbot24 2 года назад

      @@mistermhw blue indicated time?

    • @mistermhw
      @mistermhw 2 года назад

      @@humenbot24 blue line indicates pressure.

    • @humenbot24
      @humenbot24 2 года назад

      @@mistermhw What is the name of this Chart?

    • @mistermhw
      @mistermhw 2 года назад

      @@humenbot24 we usually name it barton chart or it can be hydrotest chart.

  • @n9family277
    @n9family277 2 года назад

    Keren mas

  • @cobrawins
    @cobrawins 2 года назад

    انا من مصر استطعت تصنيع واحده

    • @mistermhw
      @mistermhw 2 года назад

      Congratulation Sir, and please also help me to share my channel to another friend.

  • @andiksuharsono2490
    @andiksuharsono2490 2 года назад

    Bangga sebagai bagian dari ini semua.

  • @spears104
    @spears104 2 года назад

    did you have to return the chart recorder to the museum when you were done?

  • @nomotriutomo7720
    @nomotriutomo7720 2 года назад

    hydrotes dimana ini bosquh

    • @mistermhw
      @mistermhw 2 года назад

      PT. Boma Bisma Indra

  • @andredemunck49
    @andredemunck49 2 года назад

    Totally wrong setting not approved

    • @mistermhw
      @mistermhw 2 года назад

      Ok Sir, Thank you for your correction

  • @HTXJM
    @HTXJM 2 года назад

    Is this vessel supposed to be hydro tested at same position it will be in service?

    • @mistermhw
      @mistermhw 2 года назад

      Hydrostatic position can be done according to actual conditions in the field or in the workshop. If the service position is in a vertical condition and the hydrotest is carried out in the workshop, of course it will depend on the available space. Calculated, will be verified for hydrotest pressure using a vertical or horizontal position, which will involve gravity. Therefore, if the vessel uses an ASME stamp, the FORM U must be informed that the hydrostatic test is carried out in a vertical or horizontal position.

    • @HTXJM
      @HTXJM 2 года назад

      @@mistermhw thanks so much for the great info!

    • @mistermhw
      @mistermhw 2 года назад

      @@HTXJM ok, you're welcome

  • @SobhaSangeetaPainting
    @SobhaSangeetaPainting 2 года назад

    Nice video

  • @MrAndhiguy
    @MrAndhiguy 2 года назад

    Damn. So awesome. Wondering ago I ever done this practical colleague and now I miss those moment too.

  • @MrAndhiguy
    @MrAndhiguy 2 года назад

    Iki jenis las opo kang ? Material yg dijoint apa ?

  • @MrAndhiguy
    @MrAndhiguy 2 года назад

    Ini namanya cold working. Pekerjaan metal forming dlm kondisi suhu kamar. Nais thread pakde

    • @mistermhw
      @mistermhw 2 года назад

      Siap Juragan, bantu subscribe dan share ke yang lain. Biar semangat bikin contentnya.

  • @MrAndhiguy
    @MrAndhiguy 2 года назад

    Why we don't carry to the site part by part and fabrication on site ? It's more efficient than we carry like this.

  • @MrAndhiguy
    @MrAndhiguy 2 года назад

    Woalah iki alat e test barton. Kalau utk pressure tank (booster tank, reaktor tank, silo) brp bar ? Metode nya sama pakai yg ini jg ?

  • @caldens
    @caldens 2 года назад

    Pak ini pabriknya dimana ya

    • @mistermhw
      @mistermhw 2 года назад

      Jawa Timur pak, PT. BOMA BISMA INDRA.

  • @basicconceptsinindustry3617
    @basicconceptsinindustry3617 2 года назад

    What is Spiral Wound Gasket? Understand Application & Use #Heavy industry #Pressure vessels #pipelines ruclips.net/video/55pPq7AIAgI/видео.html

  • @duniachenel8760
    @duniachenel8760 2 года назад

    Nice

  • @mubarakdiwan7156
    @mubarakdiwan7156 2 года назад

    Mubarak diwan 🌹🇮🇳🌹

  • @u2lchannel931
    @u2lchannel931 2 года назад

    can you share to me the procedure of hydrotest?

    • @mistermhw
      @mistermhw 2 года назад

      Ok, share your email

  • @nurfariesyadamia8005
    @nurfariesyadamia8005 2 года назад

    This is not hell fire.. In islam hell fire colour was super black.